Characterization of Field Deterioration in V-Based SCR Catalysts Retrieved from an Operating Marine Vessel

Daekun Kim, Woo-Seok Jeon

Key points

From the paper's conclusion
  • These results demonstrate the value of a training vessel as a traceable longitudinal platform for linking marine operating history with catalyst deterioration.

Abstract

Marine selective catalytic reduction (SCR) systems are widely used to comply with stringent NOx emission limits, yet the long-term deterioration of catalysts under traceable real-world ship operation remains insufficiently documented. In this study, V-based SCR catalysts were recovered from the generator-engine SCR system of the training ship T/S SEGERO after approximately 1000 and 3600 h of actual vessel operation and compared with a fresh reference. The field-aged catalysts were evaluated by visual inspection, pressure-drop measurements, SEM–EDS, ICP-OES, N2 physisorption, and laboratory NH3-SCR activity testing. After 3600 h, localized carbonaceous and inorganic deposits were observed together with an approximately 9–18% increase in pressure drop relative to the fresh catalyst. Ca, P, and Zn accumulation increased with field exposure, while Ca and S showed spatial co-localization at the catalyst surface. The BET surface area decreased by approximately 10% after 1000 h and 35% after 3600 h. Relative DeNOx activity remained close to that of the corresponding fresh reference after 1000 h but was lower after 3600 h, with mean reductions of 8.3–13.3% in the first layer and 2.0–5.9% in the second layer across 300–400 °C. These results demonstrate the value of a training vessel as a traceable longitudinal platform for linking marine operating history with catalyst deterioration.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers