Tuning Lanthanum Promotion in Ni/CeO2 Catalysts for Hydrogen-Rich Syngas Production via Partial Oxidation of Methane
Wedad A. Al-onazi, Abdulaziz A. M. Abahussain, Tahani Saad Algarni, Mohammed F. Alotaibi, Mohammed O. Bayazed, Rehab M. Ali, Alaaddin M. M. Saeed, Khalid M. Alshamrani,
Key points
From the paper's conclusion- Hence, these findings reveal that 1.5 wt.% La is the optimum loading, which balances support structure, metal–support interaction, surface chemistry, and active-site accessibility, and offers a practical strategy for producing more effective and stable Ni/CeO2 catalysts for hydrogen-rich syngas production via POM.
Abstract
Partial oxidation of methane (POM) provides an efficient route to convert methane into hydrogen-rich syngas, with lower energy demands than conventional steam reforming. This work evaluates lanthanum promotion effects on the physicochemical properties and catalytic behaviour of Ni/CeO2 catalysts. A series of 5Ni + xLa/CeO2 catalysts with 0–2 wt.% La was synthesised by wetness impregnation and characterized using N2 adsorption–desorption, Raman spectroscopy, and cyclic H2-TPR–O2-TPO–H2-TPR analysis. The results proved that promoter La has a strong effect on the structure and surface chemistry of the Ni/CeO2 catalysts, as it modifies the CeO2 framework, encourages the formation of surface carbonate species, and changes Ni interaction with the support. These structural shifts are closely tied to the enhancement of the catalyst’s performance and stability during POM. Among the catalysts, 5Ni + 1.5La/CeO2 struck the best balance between textural properties and catalytic performance. At 600 °C and a GHSV of 14,400 mL h−1 gcat−1, the CH4 conversion reached about 57–59% and H2 yield reached 53–55% over 300 min on stream. It also led to more than 70% CH4 conversion and more than 65% H2 yield for 22 h at 600 °C and 7200 mL h−1 g_cat−1, showing sustainable hydrogen-rich syngas production during continuous operation. However, increasing the La loading to 2 wt.% strengthened the La–CeO2 interaction to the point of limiting the accessibility and dispersion of active sites, which lowered catalytic activity. Hence, these findings reveal that 1.5 wt.% La is the optimum loading, which balances support structure, metal–support interaction, surface chemistry, and active-site accessibility, and offers a practical strategy for producing more effective and stable Ni/CeO2 catalysts for hydrogen-rich syngas production via POM.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Effect of Promoters on Co/Al2O3 Catalysts for Partial Oxidation of Methane: Structure–Activity CorrelationsCatalysts · 2025
- Optimal Co doping to Ni-based catalyst to promote partial oxidation of methane for syngas productionChemical Engineering Journal · 2026
- Enhanced CO2 Methanation over Solution-Combustion Synthesized Ni/Kaolin Catalysts: The Effect of Fe and La Promotion.Molecules (Basel, Switzerland) · 2026
- Design of Ni-promoted Ca2Fe2O5/modified ceria as oxygen carrier for fast and carbon-resistant chemical-looping steam methane reformingApplied Catalysis B: Environmental · 2025
- Effect of La on the Structure, Selectivity and Stability of La/Co3O4 Catalysts in Preferential Oxidation of Carbon Monoxide in Hydrogen-Rich StreamsCatalysis Letters · 2026
- Optimizing LaNiO3 Perovskite as Catalyst Precursor for the Revalorization of Biogas by Dry Reforming of Methane.Molecules (Basel, Switzerland) · 2026