Mechanical and Dynamic Responses of Carbon–Innegra Hybrid Composites: Insights into Viscoelasticity and Failure Mechanisms
Ciprian Ionuț Morăraș, Teodor Adrian Badea, Cosmin Mihai Mirițoiu, Daniela-Lucia Chicet, Lucia Raluca Maier, Viorel Goanță
Key points
From the paper's conclusion- The combined tensile, DMA, vibration, and microscopic results demonstrate that the woven CI architecture strongly influences the mechanical, viscoelastic, and dynamic responses of the composite.
Abstract
Carbon–Innegra (CI) hybrid composites combine the high stiffness and strength of carbon fibers with the high deformation and energy dissipation capabilities of Innegra fibers, offering potential for lightweight structures subjected to complex mechanical and dynamic loading. This study investigates the mechanical, viscoelastic, and dynamic behavior of a woven CI hybrid composite through an integrated experimental approach. Tensile tests were performed on specimens cut along three different directions (0°, 90°, and 45°), revealing a pronounced orientation dependence of the tensile response. The average tensile strength was 239.53 MPa in the longitudinal direction, 186.84 MPa in the transverse direction, and 53.52 MPa in the diagonal direction, while the 45° specimens exhibited strains at failure of approximately 15–17.5%. Dynamic mechanical analysis (DMA) showed strong orientation dependence of the viscoelastic response. At 30 °C, the storage modulus ranged from approximately 8.7–9.9 GPa in the transverse direction and 6.1–7.6 GPa in the diagonal direction, while the maximum tan δ values were approximately 0.656–0.699, depending on specimen orientation. Free-vibration tests conducted on cantilever specimens demonstrated a clear anisotropic dynamic response. For a free length of 200 mm, the natural frequencies were 60.00 Hz, 51.28 Hz, and 32.87 Hz for the transverse, longitudinal, and diagonal orientations, respectively, while the highest damping ratio reached 0.0240 in the diagonal direction. Optical microscopy was used to examine the post-failure morphology and identify the main damage mechanisms, including yarn reorientation, delamination, reinforcement damage, and resin degradation. The combined tensile, DMA, vibration, and microscopic results demonstrate that the woven CI architecture strongly influences the mechanical, viscoelastic, and dynamic responses of the composite.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Experimental Investigation of Mode I and Mode II Interlaminar Fracture Behavior of Carbon/Kevlar‐Epoxy Based Hybrid CompositePolymer Composites · 2026
- Determination of Mechanical Properties of Single and Double-Layer Intraply Hybrid Composites Manufactured by Hand Lay-Up MethodPolymers · 2026
- Drilling Damage and Dynamic Response of Carbon/Glass Hybrid Nomex Sandwich Composites.Polymers · 2026
- Hygrothermal durability of Elium® glass–carbon hybrid laminates: Role of stacking architecture and data-driven sensitivity analysisProceedings of the Institution of Mechanical Engineers Part L Journal of Materials Design and Applications · 2026
- Impact Damage Mechanisms in Hybrid Chopped Aramid–Basalt UHMWPE Composites Under Gas–Gun LoadingPolymers for Advanced Technologies · 2026
- Oblique Quasi-Static Indentation and Residual Compressive Behavior of Hybrid Woven Composite Laminates.Materials (Basel, Switzerland) · 2026