Synergistic Performance and Microscopic Mechanism of MK-GGBS-Modified Fly-Ash-Based Alkali-Activated Pastes
Yangyi Diao, Ping Xu, Lingfeng Zhao, Lin Zhu, Wenbing Hu
Key points
From the paper's conclusion- The results showed that when the total MK-GGBS replacement level increased from 20% to 50% at a mass ratio of 1:1, the initial and final setting times decreased by 50.0% and 48.4%, respectively, the fluidity decreased by approximately 9.0%, and the compressive strength initially increased and then decreased.
Abstract
Fly ash (FA) is one of the most widely used precursors in alkali-activated materials; however, its relatively low dissolution rate under ambient conditions limits the development of early-age performance. To achieve adjustable performance of FA-based alkali-activated pastes and meet the diverse requirements of grouting engineering, metakaolin (MK) and ground granulated blast-furnace slag (GGBS) were used to partially replace FA. A two-stage mix design was adopted to investigate the effects of the total MK-GGBS replacement level and their relative proportions on the fluidity, setting time, and compressive strength of the pastes. XRD and SEM-EDS analyses were also conducted to characterize the phase composition and microstructure. The results showed that when the total MK-GGBS replacement level increased from 20% to 50% at a mass ratio of 1:1, the initial and final setting times decreased by 50.0% and 48.4%, respectively, the fluidity decreased by approximately 9.0%, and the compressive strength initially increased and then decreased. At a total replacement level of 40%, increasing the GGBS proportion from 10% to 40% reduced the initial setting time by 81.1%, whereas an appropriate increase in the MK proportion favored later-age strength development. Furthermore, the setting time exhibited a significant exponential correlation with the CaO/SiO2 molar ratio (R2 > 0.99), indicating that this ratio can serve as an important parameter for predicting the setting time of the pastes. Microscopic analysis indicated that an appropriate blending ratio favored the formation of a dense and continuous gel structure. The formation of N-A-S-H and C-(A)-S-H composite gels, as suggested by the XRD and SEM-EDS results, contributed to the densification of the gel structure and was associated with the improved paste performance. This study establishes relationships between the chemical composition and performance of MK-GGBS-modified FA-based alkali-activated pastes and proposes a performance regulation strategy that balances fluidity, setting time, and strength. The findings provide a theoretical basis for the optimized design and engineering application of low-carbon alkali-activated grouting materials.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Fresh, Mechanical, and Durability Performance of Ambient-Cured Fly Ash-Ground Granulated Blast Furnace Slag Geopolymer Concrete: Effect of Mix Design Parameters.Materials (Basel, Switzerland) · 2026
- Alkali-Activated Grouting Materials for Underground Coal Mines: A Critical Review of Rheology, Mechanical Performance, and Engineering ApplicabilityApplied Sciences · 2026
- Mix-Proportion Evaluation and Microstructural Characteristics of NaOH-Na2SO4 Composite-Activated Fly Ash-Based Grouting Materials.Materials (Basel, Switzerland) · 2026
- Synergistic Utilization of High-Volume Desulfurization Gypsum with Fly Ash and Slag in Alkali-Activated BindersCoatings · 2026
- Strength and stiffness development of one-part fly ash-bottom ash geopolymer stabilized soft clayScientific Reports · 2026
- Sustainable high-performance injection geopolymers, role of GGBFS and water-to-binder ratio in strength, microstructure, and predictive modelingScientific Reports · 2025