Buildings

The Effects of the Maximum Temperature and the Cooling Method on the Post-Fire Mechanical Properties of Structural Steel S355J2

Roman Červenka, Magdaléna Štujberová, Tomáš Klas

Key points

From the paper's conclusion
  • This paper reports an experimental program on hot-rolled structural steel S355J2 in which the maximum temperature and the cooling method were combined in a partial factorial design.

Abstract

Post-fire residual properties of steel lie outside the scope of the Eurocodes. This paper reports an experimental program on hot-rolled structural steel S355J2 in which the maximum temperature and the cooling method were combined in a partial factorial design. Forty-five flat tensile specimens from a single 4 mm plate were heated along a curve approximating ISO 834 to 700, 800 and 900 °C and cooled in an insulated chamber (3–4 °C × min−1), in still air (24 °C × min−1), by water spray (103 °C × min−1) or by immersion in water (estimated 580–1100 °C × min−1). Below the eutectoid temperature the cooling method changed the strength by less than 5% and left ductility unchanged. Above it the response was strongly non-linear: at 800 °C, the three slower regimes produced closely similar, fully ductile material, whereas immersion raised the tensile strength to 1.66 times the reference value and reduced the elongation to 24.5% of it. The transition lies between 103 and about 600 °C × min−1 and is bracketed rather than resolved. After 900 °C, quenching raised the yield strength 3.4-fold, while slow cooling left a ductile material below the grade minimum. The phase transformations are inferred from the mechanical response.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers