A Study on the Effects of Graphite Tailings Sand, Steel Fibers, and Nano-Silica on the Mechanical Properties of Concrete
Tian Bai, Pengfei Wang, Nan Shao
Key points
From the paper's conclusion- To promote the resource utilization of graphite tailings sand (GT), this study investigated the modification effects and mechanisms of GT and nano-silica (NS) on the mechanical properties of steel fiber-reinforced concrete, with steel fiber content fixed at 0.5% by volume.
Abstract
To promote the resource utilization of graphite tailings sand (GT), this study investigated the modification effects and mechanisms of GT and nano-silica (NS) on the mechanical properties of steel fiber-reinforced concrete, with steel fiber content fixed at 0.5% by volume. In this study, modified concrete was prepared by partially replacing fine aggregate with GT and incorporating steel fibers and NS. The experiments were designed with four gradients of NS content (as a percentage of cement mass): 0%, 0.5%, 1%, and 1.5%; four gradients of GT fine aggregate replacement rates: 0%, 10%, 20%, and 30%; and a fixed steel fiber content of 0.5% by volume. Through slump tests, 7-day and 28-day mechanical property tests, and elastic modulus tests—combined with scanning electron microscopy (SEM) characterization and two-factor analysis of variance—the study systematically investigated the influence of each component on concrete performance. The results indicated that in single-additive systems, the optimal dosage of NS was 1% for both 7 days and 28 days. It increased the compressive strength, split tensile strength, and flexural strength at 28 days by 13.5%, 19.48%, and 22.45%. The optimal incorporation rate of GT was 10% for both 7-day and 28-day cures; furthermore, as the incorporation rate increased, the mechanical properties of the modified steel fiber concrete showed a downward trend. For modified steel fiber concrete under dual-blending conditions, the optimal dosages of NS and GT at 7 days were 1% and 20%, respectively. At 28 days, the optimal dosages were 1% and 10%. Under dual-admixture conditions, the improvement rates for the compressive strength, split tensile strength, and flexural strength of the modified concrete at 28 days were 17.72%, 21.86%, and 24.87%. Analysis of variance (ANOVA) showed that at 7 days of curing, the effect of NS on all three mechanical strengths was highly significant (p < 0.01). At 28 days, NS remained the primary influencing factor. Microscopic analysis indicated that GT optimized the pore size distribution of the matrix through a fine-particle filling effect, while NS refined the pore structure and improved the interface transition zone between aggregates and steel fibers through pozzolanic reactions. The physical filling and chemical modification of the two factors complement each other, jointly enhancing the density of the cement matrix.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Development and performance evaluation of nano-modified polypropylene fiber-reinforced concrete using GNMPsAin Shams Engineering Journal · 2026
- Mechanical and Post-Cracking Performance of Recycled and Commercial Steel Fiber-Reinforced ConcreteApplied Sciences · 2026
- Functional upcycling of nanomodified cementitious waste into recycled aggregate with multiscale reinforcement and environmental performance assessment.Environmental research · 2026
- Mechanical Properties, Microstructure, and Water Absorption of Concrete Reinforced with Surface-Treated Basalt Fibers and NanosilicaBuildings · 2026
- Sustainable construction from industrial waste: synergistic stabilization of granite residual soil using red mud byproduct and nano-silicaResults in Engineering · 2026
- Application of Graphite Tailings in Concrete Manufacturing: A ReviewMaterials · 2026