Assessing the Durability of Oil Shale Ash as a Partial OPC Replacement in Mortar: A Study on Mechanical Properties Under Sulfate
Walid Fouad Edris, Heba Mohammad Mhedat, Mahmoud Al-Tamimi, Abd Al-Kader A. Al Sayed, Tarek Ibrahim Selouma
Key points
From the paper's conclusion- The results indicate that while moderate OSA replacement (up to 20%) may be viable under sulfate exposure, 30% replacement leads to significant deterioration.
Abstract
This research aims to investigate the durability and behavior of Jordanian oil shale ash (OSA) as a substitute material for ordinary Portland cement (OPC) and Portland Pozzolana cement (PPC) in mortar under sulfate attack. Mortar samples with replacement ratios of 0%, 10%, 20%, and 30% of OSA were utilized in this investigation. The study is divided into two stages. In the first stage, the effect of OSA replacement on the mechanical properties and hardening time of mortar samples is examined over a curing period of 3, 7, 14, and 28 days using potable water. The second stage focuses on studying the durability of mortar samples with the aforementioned OSA replacement ratios. These mortar samples are fully immersed in a sodium sulfate solution with a concentration of 5% and subjected to wet and dry cycles for degradation at 1, 6, 12, 18, 24, 30, and 36 days. Various analyses were conducted, including compressive strength testing, SEM analysis, mass loss measurement, ultrasonic pulse velocity assessment, relative dynamic modulus of elasticity (RDME) evaluation, and visual inspection. For OPC-based mortars, compressive strength ranged from 44.00 to 49.75 MPa (0% OSA), 42.88 to 48.29 MPa (10% OSA), 44.50 to 50.88 MPa (20% OSA), and 31.00 to 36.53 MPa (30% OSA). For PPC-based mortars, compressive strength ranged from 36.00 to 42.32 MPa (0% OSA), 39.73 to 43.60 MPa (10% OSA), 44.97 to 46.06 MPa (20% OSA), and 22.35 to 28.18 MPa (30% OSA). Specimens with 0%, 10%, and 20% OSA showed continued increases in compressive strength, UPV, and RDME throughout exposure, while 30% OSA specimens showed deterioration after 24 days (OPC) and 18 days (PPC), with mass losses increasing from 0.52% to 8.4% (OPC) and 0.75% to 7.8% (PPC). The results indicate that while moderate OSA replacement (up to 20%) may be viable under sulfate exposure, 30% replacement leads to significant deterioration. However, the absence of non-sulfate controls prevents definitive separation of continued hydration from sulfate resistance. These findings provide practical guidance for the use of OSA in sulfate-prone environments.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Nitrogen Adsorption Measurement for Pore Structure Characterisation of Cement–Oil Shale Ash Composite Exposed to an Aggressive Salt EnvironmentMaterials · 2026
- Sustainable mortar production using volcanic ash and crushed laterite as partial cement replacementsCement · 2025
- Optimization Techniques for High-Rate Utilization of Bottom Ash and Marble Dust in Green TechnologiesBuildings · 2026
- Performance Evaluation of Pozzolanic Cements Versus Ordinary Portland Cement: Mechanical, Durability, and Compositional Insights at the Paste and Mortar ScaleBuildings · 2026
- Mechanical performance, durability, and hydration characteristics of binary and ternary blended mortars incorporating waste glass powder and Ethiopian scoriaDiscover Concrete and Cement · 2026
- Assessment of sulfate resistance in cementitious systems incorporating low-grade calcined kaolinite clay and limestoneJournal of Sustainable Cement-Based Materials · 2025