Thermal Deformation of External Wall Insulation Systems Using EPS, XPS and PU Boards: A Combined Numerical and Experimental Study
Li Li, Jiayou Liu, S Y Li, Junhao Song, Xin Li, Li J
Shandong University of Science and Technology · Shanghai Urban Construction Design and Research Institute (Group)
Abstract
Under extreme steady-state temperature gradients, external thermal insulation composite systems (ETICSs) are prone to thermal deformation, which can cause mortar cracking, hollowing, and even delamination and detachment of insulation boards, thus degrading building envelope performance and threatening structural and personal safety. In this study, a combined method of numerical simulation using ANSYS software and experimental testing was adopted to investigate the thermal deformation characteristics of three commonly used insulation materials: Expanded Polystyrene (EPS), Extruded Polystyrene (XPS), and Polyurethane (PU). The effects of temperature difference from 10 °C to 30 °C, insulation board thickness from 30 mm to 100 mm, and surface mortar thickness from 5 mm to 10 mm on strain distribution and deformation mechanism were systematically analyzed. Experimental validation showed good agreement with the simulation results, quantified by an estimated relative error of less than 15% across the investigated insulation thicknesses and steady-state temperature conditions. The results indicate that the strains of EPS, XPS, and PU boards all increase significantly as the temperature difference across the board rises. Under outdoor temperatures of 30 °C, 40 °C and 50 °C with a constant indoor temperature of 20 °C, the thickness-direction strain at the EPS–mortar interface increases by approximately 35% when the temperature difference increases from 10 °C to 30 °C. Increasing both insulation board thickness and mortar protective layer thickness effectively reduces thermal deformation. Specifically, when the EPS board thickness increases from 30 mm to 100 mm, the thickness-direction strain decreases by approximately 73%; and when the mortar thickness increases from 5 mm to 10 mm, the interfacial strain decreases by approximately 32%. Due to differences in linear expansion coefficients, the three insulation materials exhibit distinctly different thermal deformation behaviors, with the thickness-direction strain following the order EPS > XPS > PU. These findings provide a theoretical basis and data support for material selection, structural optimization, and safety design of external wall insulation systems.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- TOPSIS-Based Selection of Materials for the Internal Insulation of Heritage BuildingsMaterials · 2026
- Deterioration of physical and mechanical properties of tunnel insulation materials under water–salt immersion and freeze–thaw cyclesCase Studies in Thermal Engineering · 2025
- Investigation of the probability of losses in the external insulation layer of residential engineering projects using the weather test.Science progress · 2026
- Uncertainty-aware determination of thermal transmittance and systematic evaluation of insulation retrofit scenarios for energy-efficient building envelopeJournal of Thermal Analysis and Calorimetry · 2026
- Hygrothermische Charakterisierung und Bewertung eines innovativen Aerogel‐basierten Wärmedämmputzesce/papers · 2026
- Einfluss von Temperatur und Alterung auf das Verhalten von PU‐SandwichelementenStahlbau · 2026