Effect of Zein-Coated Magnesium Oxide Nanoparticle Incorporation on the Shear Bond Strength of Different Resin Composites After Thermocycling.
Ghada H Naguib, Rabab Aljawi, Sarah Alqarni, Dina Alsharif, Jumana Mazhar, Abeer Alnowaiser, Mohamed T Hamed
Department of Restorative Dentistry, Faculty of Dentistry, King Abdulaziz University, Jeddah 21589, Saudi Arabia. · Department of Pediatric Dentistry, Faculty of Dentistry, King Abdulaziz University, Jeddah 21589, Saudi Arabia.
Key points
From the paper's conclusion- Conclusions: Adding zMgO NPs to resin composites improved SBS after thermocycling, with material- and concentration-dependent differences in failure-mode analysis.
Abstract
OBJECTIVES: Studies have shown that nanoparticles can impart beneficial properties when integrated into resin composites; however, it remains unclear how this affects shear bond strength. This study aimed to evaluate the effects of composite formulation and zein-coated magnesium oxide nanoparticle (zMgO NP) concentration on shear bond strength (SBS) and failure mode following thermocycling. METHODS: A total of 180 extracted human molars were randomly allocated among four composite formulations and three zMgO NP concentrations (0%, 0.5%, and 1%; n = 15). Composite cylinders were bonded to prepared dentin surfaces and thermocycled for 10,000 cycles between 5 °C and 55 °C. SBS was analyzed using two-way ANOVA and post hoc multiple comparisons with Tukey's test. Failure modes were assessed stereomicroscopically and analyzed using the chi-square test. RESULTS: The SBS of the modified composites in all groups significantly increased, with the 0.5% zMgO NP groups exhibiting the highest SBS. The 0.5% zMgO NPs N-Ceram group had the highest SBS overall. The unmodified Z350 composite exhibited the highest adhesive failure, while the control N-Flow composite demonstrated the highest cohesive failure. The modified conventional and flowable composites showed initially lower adhesive failure, which increased progressively as zMgO NPs increased. The bulk-fill composite initially showed higher adhesive failure, with the 0.5% group demonstrating lower adhesive failure and the 1% group exhibiting increased adhesive failure. CONCLUSIONS: Adding zMgO NPs to resin composites improved SBS after thermocycling, with material- and concentration-dependent differences in failure-mode analysis. Further validation studies are needed to verify clinical viability.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Influence of zein-coated magnesium oxide nanoparticle reinforcement on the flexural strength of polymeric denture base resins.Frontiers in dental medicine · 2026
- Synergistic modification with silanized MgO nanoparticles and MAP-POSS enhances mechanical performance and antibacterial activity of dental composite resins.Journal of the mechanical behavior of biomedical materials · 2026
- Effect of magnesium oxide nanoparticles on the flexural strength, surface roughness, and color of self-cure PMMA provisional crownsScientific Reports · 2026
- Influence of zinc-modified niobium nanoparticles incorporation in resinous monomers on mechanical properties.Brazilian dental journal · 2026
- The Influence of Filler Morphology and Loading Level on the Properties of Light-Curing Dental CompositesDentistry Journal · 2026
- Niobium-Doped Nanofiber Reinforcement of Low-Viscosity Bulk-Fill Resin Composites: Physicomechanical Properties and Mineral Deposition Potential.Polymers · 2026