A Post-Processing Framework for Crack–Hole Interaction: Amplification, Deflection, and Capture Across Eight Geometries
Abdulnaser M. Alshoaibi, Yahya Ali Fageehi
Key points
From the paper's conclusion- The framework combines a matched-pair hole amplification factor Λ (the mode-I stress-intensity ratio with and without holes at equal crack extension), a steering angle reconstructed from KI and KII, a three-regime classification (capture, deflection and escape, hole switching), and a distinction between geometric and mechanical arrest.
Abstract
Holes are widely proposed as crack arrestors, but crack-growth simulations usually report the crack path without defining arrest in a linear-elastic model or explaining its mechanism. This paper proposes a post-processing framework for crack–hole interaction and applies it to previously reported ANSYS SMART simulations of eight hole-bearing geometries. The framework combines a matched-pair hole amplification factor Λ (the mode-I stress-intensity ratio with and without holes at equal crack extension), a steering angle reconstructed from KI and KII, a three-regime classification (capture, deflection and escape, hole switching), and a distinction between geometric and mechanical arrest. In the three-point-bending beam the perforated crack ends at the middle hole although KI is 1.6–2.1 times that of the hole-free beam, so termination reflects capture, not relief; the four-point-bending specimen gives Λ ≈ 1.1–1.5. Handbook-based estimates for the modified CT specimens and the one-hole plate also exceed 1, but the source data for these cases are inconsistent, so the estimates are indicative only and are not counted as evidence. A persistent sign of KII identifies the capturing hole in the notched plate and CT specimens, and a 0.8 mm shift in the pre-crack changes the hole captured; this sensitivity comes from single runs and has not yet been checked for numerical convergence. A reporting protocol specifies the further runs needed, including convergence checks of the crack path and a hole-free twin of the modified CT specimen. The conclusions rest on signs, trends and ratios and are testable hypotheses, not a universal arrest criterion.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- A Three-Level Global-Local Coupling Strategy with Non-Matching Interfaces for Crack Propagation Analysis in Beam-Solid StructuresApplied Sciences · 2026
- An Investigation on Crack bridging in Metal Matrix Composite using Analytical and Numerical ApproachesEngineering Research Express · 2026
- Phase‐Field Modeling of Borehole‐Pressure‐Induced Fracture Propagation in Coal‐Rock Composites Considering Compressive‐Shear Failure and Interface EffectsFatigue & Fracture of Engineering Materials & Structures · 2026
- Designed intermittency in interlaminar fracture via kirigami-induced crack-front wideningComposites Science and Technology · 2026
- Energy-efficient fracturing based on stress-coupled perforationPetroleum Science · 2026
- Influence of controlled interior defect morphology on tensile fracture behavior of binder jetting additively manufactured 17-4PH stainless steelJournal of Materials Research and Technology · 2026