Anchorage Degradation and Failure Mechanisms of Self-Swelling Split-Sets Under Corrosive Underground Mine Environments
Menglong Huang, Shuai Xu, Fidelis Suorineni, Donghui Li, Zhengming Yang, Qingyu Zhu
Key points
From the paper's conclusion- The findings support durability assessment and ground-support selection under the investigated corrosive laboratory conditions.
Abstract
Corrosion-induced degradation remains a major limitation to the long-term performance of frictional ground-support elements in underground mines, yet the durability of recently developed self-swelling Split-sets remains poorly understood. This study investigates their time-dependent anchorage response under a non-corrosive air control, pure water, pH 3 H2SO4 solution, and 6 wt.% Na2SO4 solution for up to 90 d using pull-out tests, apparent mass loss measurements, X-ray diffraction analysis and scanning electron microscopy. Under aqueous exposure, a distinct two-stage response was observed: mean peak load increased during the first 14 d and subsequently decreased with prolonged exposure. After 90 d, mean peak load decreased by 24.71%, 30.52%, and 38.59% in pure water, pH 3 H2SO4, and 6 wt.% Na2SO4, respectively, relative to the 90 d non-corrosive air control. At later exposure durations, aqueous exposure also shifted the governing failure mode from steel-tube rupture to interfacial sliding. Under aqueous exposure, semi-quantitative XRD estimates of relative Ca(OH)2 content increased during the first 14 d and subsequently decreased, while mean apparent mass loss generally increased. Nevertheless, 90 d mean peak loads remained approximately 3.95–4.87 times those of conventional Split-sets and 1.24–1.48 times those of grouted Split-sets. These results are consistent with a combined influence of early hydration-related strengthening and subsequent exposure-induced degradation; however, the individual contributions of steel corrosion and self-swelling-agent deterioration were not separately quantified. The findings support durability assessment and ground-support selection under the investigated corrosive laboratory conditions.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- An Experimental Investigation of the Effects of Dry–Wet Cycles and pH Values on Gangue Waste-Based Roadway Shotcrete: Mechanical Performance and Microstructural AnalysisApplied Sciences · 2026
- Acid-Induced Mechanical Degradation and Microstructural Damage of Shield Muck Solidified with ESCA and P.O 42.5 Cement.Materials (Basel, Switzerland) · 2026
- Fracture Behavior and Crack Propagation Processes of Composite Structure of Goaf Backfill and Roof Rock Based on Acoustic Emission MonitoringProcesses · 2026
- Hydro-Mechanical Degradation and Progressive Failure of Sandstone–CGFB Composite Structures Under Cyclic Water Immersion: Implications for Water-Induced Instability Risk in Backfilled GoafsApplied Sciences · 2026
- Numerical Investigation of Deformation and Reinforcement in an Alkaline Water-Affected Coal-Seam Roadway Section Within Inclined StrataSymmetry · 2026
- Degradation Mechanisms of Concrete in Underground Coal Mine Water Tanks Subjected to Sulphate AttackApplied Sciences · 2026