Acoustic Nonlinearity as an In-Situ Indicator of Yield Onset in S235 Structural Steel Under Monotonic Tensile Loading
Alexandros S. Tiktapanidis, Theodoti Z. Kordatou, Spyridoula G. Farmaki, Dimitrios A. Exarchos, Theodore E. Matikas
Key points
From the paper's conclusion- This study investigates the continuous, in-situ evolution of the second-order acoustic nonlinearity parameter (β2) throughout the monotonic tensile response of S235 structural steel, from the elastic regime to fracture.
Abstract
The residual life of metallic structures is dictated by microstructural plastic damage, which conventional linear ultrasonics often fail to detect early. This study investigates the continuous, in-situ evolution of the second-order acoustic nonlinearity parameter (β2) throughout the monotonic tensile response of S235 structural steel, from the elastic regime to fracture. Bulk longitudinal waves were excited by a contact piezoelectric transducer and detected through-thickness using a non-contact Laser Doppler Vibrometer on a notched specimen. This allowed the normalized acoustic parameters to be mapped directly onto the macroscopic stress-strain curve. Three distinct acoustic regimes were identified. Up to the onset of the yield plateau, the nonlinearity parameter and the linear attenuation remained at unity within the specimen-to-specimen scatter. Beyond the yield point, β2/β2(0) rose steeply to approximately 4.5, whereas the normalised attenuation increased by at most approximately 20%. The rise extended over the yield plateau of the stress–strain curves and the parameter saturated when work hardening resumed (nominal strain ≈ 0.031–0.033), ahead of the maximum load (≈0.043); a lower value was recorded only at the last acquisition, at which the signal quality was degraded. The departure of β2 from unity, i.e., the first increase of the second-harmonic amplitude, occurred between nominal strains of 0.015 and 0.021, coinciding with the onset of the yield plateau (≈0.017) and slightly above the 0.2% offset yield strain (0.0128 ± 0.0004), as expected for a notched specimen in which plasticity reaches the interrogated volume once it spreads across the ligament; this supports its potential as a marker of yield onset. The increasing trend provides a continuously acquired ferritic-pearlitic reference data set and is consistent with, although not by itself proof of, a governing role of the initial dislocation substructure in harmonic generation.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Rayleigh wave second harmonic generation and mixing for probing depth-varying acoustic nonlinearity in thermally damaged steel.Ultrasonics · 2026
- Exploratory Stage-Resolved Acoustic Emission Characterization During Tensile Testing of Furnace-Exposed S235 Structural Steel.Materials (Basel, Switzerland) · 2026
- Multi-Mode Nonlinear Ultrasonic Characterization of Fatigue Crack Evolution in GH4169 Nickel-Based Superalloy.Materials (Basel, Switzerland) · 2026
- Mechanically Referenced Early Acoustic Emission Indicators of Thermally Modified Deformation in S235 Structural Steel.Materials (Basel, Switzerland) · 2026
- Residual-stress distribution in gear journal shafts induced by mechanical roll hardeningMechanical Sciences · 2026
- In Situ Investigation of Crystallographic Effects on Short Fatigue Crack Propagation From Surface Notches in a High‐Strength Alloy Structural SteelFatigue & Fracture of Engineering Materials & Structures · 2026