Key points
From the paper's conclusion- The material removal volume (MRV), electrode wear volume (EWV), and machining depth were evaluated and compared with those obtained using conventional single-material cylindrical electrodes made of Cu, Al6061 and SKD11.
Abstract
Electrode materials and discharge parameters play critical roles in determining the machining efficiency and precision of electrical discharge machining (EDM). Conventional EDM generally employs a single electrode material, which may limit discharge performance and the surface characteristics of the machined workpiece. This study developed a multi-material composite electrode (MMCE) using materials with different melting points, electrical conductivities, and thermal conductivities. The MMCE was designed to develop a stepped end-face profile through differential wear of its constituent materials during rotating EDM. This profile, combined with electrode rotation, may facilitate dielectric circulation and debris evacuation. The MMCE consisted of three one-third sector-shaped cylindrical segments made of copper (Cu), aluminum alloy (Al6061), and mold steel (SKD11), respectively, forming a cylindrical electrode with a diameter of 20 mm. Pulse duration, peak current, and duty factor were selected as experimental parameters. The material removal volume (MRV), electrode wear volume (EWV), and machining depth were evaluated and compared with those obtained using conventional single-material cylindrical electrodes made of Cu, Al6061 and SKD11. The experimental results revealed differential wear among the MMCE segments, resulting in a stepped electrode end-face profile. This profile, combined with electrode rotation, may facilitate dielectric circulation and debris evacuation, potentially contributing to improved EDM process stability. At a duty factor of 0.5, the MMCE achieved an MRV approximately 98% of that obtained with the Cu electrode, while its EWV was approximately three times higher. Furthermore, energy-dispersive X-ray spectroscopy detected Cu and Al on the machined surface, supporting the transfer of electrode-derived elements to the workpiece and indicating the potential of the MMCE to modify surface composition during rotating EDM.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Comparative analysis of copper and graphite electrodes in EDM of Al–SiC metal matrix compositesScientific Reports · 2026
- A Combined Taguchi–ANOVA and Deep Learning Approach for Optimizing Die-Sinking EDM of Pentagonal Cavities over EN-24 Alloy SteelEngineering Research Express · 2026
- EDM machinability and surface characterisation of Al-SiC metal matrix composites: ANOVA based response surface studyNext Materials · 2026
- A Grooved Hollow Abrasive Electrode for High-Efficiency Grinding-Aided Electrochemical Discharge Machining of SiCp/Al Metal Matrix Composites.Micromachines · 2026
- Influence of conductive powders on surface characteristics in EDM: an experimental study using desirability optimizationJournal of the Mechanical Behavior of Materials · 2026
- Electro-thermal surface evolution in EDM of dissimilar stainless-carbon steel welds: parametric effects and micro-texture correlations.Scientific reports · 2026