Masked Stereolithography of a Metacarpal Fixation Plate Prototype with a Low-Temperature Barium Titanate Coating
Eduard G. Tuns, Razvan Pǎcurar, Mircea Nǎsui
Key points
From the paper's conclusion- This study presents the design, fabrication, and preliminary characterisation of a low-profile, BaTiO3-coated dorsal fixation plate prototype for the fifth metacarpal bone.
Abstract
Fifth metacarpal shaft fractures account for a large share of hand trauma and often require operative internal fixation, yet conventional dorsal plates and cannulated screws present a stiffness mismatch with native bone and the insertion of screws can shear surface coatings. This study presents the design, fabrication, and preliminary characterisation of a low-profile, BaTiO3-coated dorsal fixation plate prototype for the fifth metacarpal bone. A curved, 0.5 mm plate was modelled in SolidWorks and overlaid with a randomised Delaunay lattice in Meshmixer, achieving 73.6% porosity with a 70% mesh reduction strategy. A linear static finite element study of a simplified periodic surrogate of the plate (nominal polymer properties, 300 N load) is reported only as an illustrative response, not as evidence of mechanical suitability. Plates were manufactured by masked stereolithography in a water-washable resin not intended for implantation (not MED610), with an average accuracy of 98.77% on three features measured before coating; the dimensions after the 120 °C and 180 °C coating steps were not remeasured. A barium titanate precursor was synthesised via the propionate route and deposited through a three-cycle, low-temperature (120 °C) submersion process followed by a solvothermal treatment at 180 °C for 1 h. Optical microscopy and SEM/EDS showed qualitative surface coverage with barium and titanium and open pores, and XRD showed reflections consistent with perovskite BaTiO3; the polymorph, thickness, adhesion, uniformity and mechanical stability of the coating were not quantified. Under cyclic compressive loading (1–2 N), a coated plate dried at 120 °C, before the solvothermal step was introduced, generated an alternating open-circuit voltage of 0.62 ± 0.08 V at 1 N and 0.93 ± 0.10 V at 2 N (peak-to-peak), much larger than that of an uncoated plate; its origin remains to be established. This is a fabrication and preliminary characterisation study of a non-biocompatible prototype: mechanical testing of the printed structure, poled and replicate electrical measurements, and biological evaluation have not yet been performed and are the next steps.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Design and Manufacturing Process of 3D-Printed Metamaterial Calcaneal Plates via Scalar Field-Driven Porous Structure FusionACS Biomaterials Science & Engineering · 2026
- Sacrificial-Template Fabrication of Orientation-Controlled Porous Titanium Lattices With Bioactive Surfaces.Small (Weinheim an der Bergstrasse, Germany) · 2026
- Biomechanical and Hydrodynamic Characterization of Gradient-Porosity Triply Periodic Minimal Surfaces Polyether Ether Ketone Scaffolds for Craniofacial Bone Defect Repair.The Journal of craniofacial surgery · 2026
- Fused filament fabrication of radiopaque barium sulfate-reinforced polyetheretherketone composites for thin-walled patient-specific orbital reconstruction.Journal of materials science. Materials in medicine · 2026
- Volumetric Infiltration of Brushite and Monetite Cements into Laser Powder Bed Fusion Ti-6Al-4V Lattices: A Feasibility Study of Lattice Geometry and Cement Formulation.Materials (Basel, Switzerland) · 2026
- Early-stage stability and degradation of patient-specific biodegradable 3D-printed implants for critical mandibular reconstructionDental Materials · 2026