High-Strength Recycled Concrete: Hybrid Material Evaluation and Predictive Modeling
Mahmoud Atif Nsour, Ahmed Hasan Alwathaf
Key points
From the paper's conclusion- These findings identify 34% RCA as the highest replacement level tested at which the ACI 363R threshold was met, and provide criterion-specific, statistically grounded design guidance for structural RAC within the tested range.
Abstract
The demand for sustainable construction has intensified the search for structurally viable recycled concrete aggregate (RCA) applications, historically limited by high water absorption, low density, and a weak dual interfacial transition zone (ITZ). This study experimentally evaluates mix designs using supplementary cementitious materials (SCMs) and fibres against the ACI 363R high-strength threshold (55 MPa) at a low water-to-cementitious (w/c) ratio of 0.32. Seventeen mixes were evaluated across three RCA replacement levels (0%, 34%, 67% by weight) containing fly ash (FA: 15%, 25%), silica fume (SF: 7%, 15%), polypropylene fibres (300, 600 g/m3), and steel chips (3.75 kg/m3). One-way analysis of variance (ANOVA) and Welch pairwise t-tests confirmed a statistically significant effect of RCA replacement level on 28-day compressive strength (F(2,6) = 382.3, p < 0.001); at 67% RCA, no mix reached 55 MPa (maximum 46.45 MPa). At 34% RCA, 25% FA achieved a 28-day strength of 59.00 MPa, not significantly different from the natural-aggregate control (p = 0.356). SF15% combined with steel chips yielded the highest flexural (9.90 MPa) and splitting tensile (5.51 MPa) strengths, an improvement over the plain 34% RCA baseline. Based on indirect durability indicators, SF7% showed the most favourable ultrasonic pulse velocity (UPV = 4.59 km/s) and lowest water absorption among the 34% RCA mixes. All mixes maintained placement viability (slump > 85 mm) at 1.3% superplasticizer. A multiple linear regression (MLR) model calibrated on the 17-mix dataset predicted 28-day compressive strength (R2 = 0.874, RMSE = 2.03 MPa): f’c (MPa) = 61.35 − 0.265·RCA (%) + 0.169·FA (%) + 0.119·SF (%), in which the RCA and FA terms are statistically significant but the SF term is not. These findings identify 34% RCA as the highest replacement level tested at which the ACI 363R threshold was met, and provide criterion-specific, statistically grounded design guidance for structural RAC within the tested range.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Influence of High-Performance Recycled Aggregates on Mechanical Properties of High-Strength ConcreteInfrastructures · 2026
- Thermal and mechanical behaviour of high-performance concrete incorporating recycled concrete aggregateConstruction and Building Materials · 2026
- Development of High-Performance Eco-Friendly Concrete Incorporating Recycled Fine Aggregates: Mechanical, Microstructural and Carbon Footprint AssessmentBuildings · 2026
- Evaluation of properties and in situ strength of recycled aggregates concreteMultiscale and Multidisciplinary Modeling Experiments and Design · 2026
- Performance evaluation of fibre-reinforced treated recycled aggregate concrete incorporating rice husk ash using a two-stage mixing processInnovative Infrastructure Solutions · 2026
- Experimental and sustainability-driven engineering assessment of recycled concrete aggregates: mechanical performance, durability, environmental and economic implicationsFuture Technology · 2026