Toward Durable Infrastructure: A Review of Self-Healing Geopolymer Concrete for Sustainable Construction
Md. Toriqule Islam, Bidur Kafle, Riyadh Al-Ameri
Deakin University
Key points
From the paper's conclusion- By integrating appropriate healing agents into geopolymer concrete, this research aims to advance a sustainable approach to durable infrastructure.
Abstract
The manufacturing process of ordinary Portland cement (OPC) is highly resource-intensive and significantly contributes to global CO2 emissions, thereby exacerbating global warming. In this context, researchers are progressively adopting geopolymer concrete owing to its environmentally friendly production process. However, cracks in OPC and geopolymer concrete structures can substantially reduce their lifespan by exposing reinforcement to the external environment, resulting in concrete deterioration. To mitigate these issues, the self-healing capability of concrete presents an innovative solution to restore structural integrity and minimise maintenance costs. This research delineates various healing techniques and their efficacy for geopolymer concrete, including crystalline admixture, fibres, bacteria, and enzymes. This study primarily examines geopolymer compositions to assess the self-healing efficiency of different healing agents. As many healing agents, including crystalline admixtures and enzyme-based systems, were originally developed for OPC-based concrete and remain underexplored in geopolymers, parallel investigations on OPC systems are also conducted to enable a comparative understanding of the underlying healing mechanisms. The current state of research indicates that crystalline admixture was unable to facilitate crack healing within the geopolymer matrix unless an additional 10% Ca(OH)2 was incorporated into the binder. The inclusion of fibres embedded with healing agents markedly improved the healing efficiency, achieving a crack width of up to 800 µm when utilised with natural fibres and bacteria. The integration of an optimal quantity of various healing agents enhances the compressive, split tensile, and flexural strength of the concrete. The optimal dosages for the crystalline admixture ranged from 1% to 1.5% by weight of the binder, while the concentration of bacteria ranged from 105 to 107 cells/mL. Furthermore, this review delineates the practical applications and limitations of various healing agents. By integrating appropriate healing agents into geopolymer concrete, this research aims to advance a sustainable approach to durable infrastructure.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Preparation and characterization of self-cured geopolymer binder using metakaolin precursorScientific Reports · 2026
- Advances in Self-Healing Ordinary Portland and Geopolymer Cement Systems: A Comprehensive Review of Stimuli-Responsive Polymer Mechanisms and PerformanceJournal of Advanced Concrete Technology · 2026
- Synergistic effect of polyvinyl alcohol fibers and spindle-like calcium carbonate on the mechanical properties and drying shrinkage of geopolymer concreteConstruction and Building Materials · 2025
- Natural Clay in Geopolymer Concrete: A Sustainable Alternative Pozzolanic Material for Future Green Construction—A Comprehensive ReviewSustainability · 2025
- Interpretation of Preferable Curing Conditions in the Realization of Durable Self-Compacting Geopolymer ConcreteJournal of structural design and construction practice. · 2026
- Flexural and fracture properties of geopolymer concrete with delithiated β-spodumeneEngineering Fracture Mechanics · 2026