Fatigue behaviour of CARALL fibre metal laminates machined by abrasive waterjet
Gianluca Parodo, Costanzo Bellini, Vittorio Di Cocco, Francesco Iacoviello, Giuseppe Moffa, Luca Sorrentino, Sandro Turchetta
Key points
From the paper's conclusion- A pressure of 300 MPa was therefore adopted for the specimens subsequently subjected to fatigue testing.
Abstract
Carbon fibre-reinforced aluminium laminates (CARALLs) combine the high specific stiffness of carbon-fibre composites with the ductility and damage tolerance of aluminium alloys, although their mechanical performance is strongly influenced by the integrity of the metal-composite interfaces and by the manufacturing route adopted for specimen preparation. In this work, CARALL laminates consisting of AA2017 aluminium sheets, CYCOM® 950-1 carbon/epoxy prepreg and 3M™ Scotch-Weld™ AF 163-2 structural adhesive films were manufactured by hand lay-up, vacuum bagging and oven curing. Specimens were subsequently extracted by abrasive waterjet (AWJ) cutting. Preliminary cutting trials were performed at water pressures of 100, 200 and 300 MPa while keeping the remaining process parameters constant. At the lower pressure levels, extensive delamination and interfacial separation were observed. At 200 MPa, some specimens appeared macroscopically intact, although SEM observations revealed local debonding at the aluminium-adhesive interface and delamination within the CFRP sublaminate. A pressure of 300 MPa was therefore adopted for the specimens subsequently subjected to fatigue testing. The results highlight the sensitivity of CARALL laminates to AWJ-induced damage and underline the importance of controlling specimen edge integrity when assessing their fatigue response.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Investigation of the effect of surface treatments on the shear performance of CFRP/Ti–6Al–4V single-lap adhesive jointsJournal of Adhesion Science and Technology · 2026
- Bio-Inspired Optimization of AWJM Parameters for Enhanced Machining of Glass and Carbon Fiber-Reinforced Composites.ACS omega · 2026
- Multiscale Transfer of Cohesive-Zone Parameters for Opening-Dominated Interlaminar Fracture in Carbon-Fiber-Reinforced Aluminum Laminates.Polymers · 2026
- Increasing Adhesive Layer Thickness Reduces Ultimate Load Capacity in Double-Lap CFRP-to-Steel Joints.Materials (Basel, Switzerland) · 2026
- Effects of laser processing parameters and scanning angle on damage morphology and residual tensile properties of CFRP laminates with a continuum damage mechanics model.PloS one · 2026
- Coating Deposition of Aldehyde‐Ketone Resin Onto Carboxylated Carbon Fibers: Surface Chemistry, Micro‐Morphology, Wettability, Monofilament Mechanical and Interfacial Shear PropertiesPolymer Composites · 2026