Decoupled pre-freeze properties and earlier freeze–thaw deterioration in RDP–defoamer-modified joint-filling mortar
Wenjie Xiao, Xiaozhang Wang, Cheng Qian, Leilei Han
Key points
From the paper's conclusion- For similar RDP-modified joint-filling mortars, the results support combining pre-freeze properties with deterioration trajectories and residual mechanical capacity when assessing freeze–thaw durability.
Abstract
Redispersible polymer powder (RDP) and defoamers are widely used to tune the workability and hardened response of cementitious mortars, but favorable pre-freeze indicators do not necessarily translate into freeze–thaw durability. This study examined a polypropylene-fiber-reinforced joint-filling mortar for prefabricated pavement bases using reference (REF), RDP-modified (RDP), defoamer-modified (DF), and combined RDP–defoamer (RDP–DF) formulations, with a commercial grout as an external benchmark. The primary comparison was between RDP and RDP–DF: both mixtures contained 280 kg m -3 mixing water and differed by the incorporation of 0.15% defoamer by binder mass. Pre-freeze mechanical, transport, and volume-stability responses were characterized, followed by longitudinal freeze–thaw tracking using mass loss and relative dynamic elastic modulus (RDEM) and by residual mechanical evaluation. Relative to RDP, RDP–DF reduced water absorption and 28-day drying shrinkage by 46.0% and 50.0%, while secant modulus increased by approximately 23%. Flexural and compressive strengths decreased by 28.8% and 25.4%, and permeability did not improve. After 15 freeze–thaw cycles, mass loss increased from approximately 0% to 5.48% and RDEM decreased from 83.94% to 64.59%. The median first observed cycle at which mass loss reached or exceeded 5% decreased from 50 to 15 cycles. In an independent 15-cycle batch, post-freeze–thaw compressive strength was 23.8 MPa for RDP and 17.2 MPa for RDP–DF, a difference of −27.7%. For similar RDP-modified joint-filling mortars, the results support combining pre-freeze properties with deterioration trajectories and residual mechanical capacity when assessing freeze–thaw durability.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Decoupled Mechanical and Surface Deterioration Trajectories of Cement Mortars with Different Fine Aggregates Under Freeze-Thaw Exposure.Materials (Basel, Switzerland) · 2026
- Influential Mechanism Analysis of Modified Absorbent Polymer in Roller-Compacted Cementitious MaterialsJournal of Materials in Civil Engineering · 2025
- Degradation behavior of early-age frozen mortar under the combined effects of sulfate attack and freeze-thaw cyclesConstruction and Building Materials · 2025
- Effects of RAP Asphalt Mortar Migration on the Cracking Performance of Recycled Asphalt Mixtures: Evaluation, Mechanism, and Regulation Strategy.Materials (Basel, Switzerland) · 2026
- Polymer-modified cement-based materials for airport pavement repair: Enhancement of interfacial bonding and freeze-thaw resistanceConstruction and Building Materials · 2025
- Experimental Investigation on Flexural Behavior of Desert Sand Concrete Beams Subjected to Freeze–Thaw CyclesMaterials · 2026