Influence of alkali activator modulus on mechanical properties and microstructure of slag-fly ash geopolymer-solidified dredged sludge
Yulin Wang, Yan Tian, Sisi Fang, Xianding Guo, Yating Fan, Jun Wang, Daohe Wu, Yinghua Cui,
Key points
From the paper's conclusion- These findings show that controlling activator modulus is important for tailoring the mechanical response and microstructure of slag-fly ash geopolymer-solidified dredged sludge.
Abstract
This study investigates the solidification of dredged sludge using a slag-fly ash geopolymer to promote its resource-oriented reuse as a sustainable construction material. Moving beyond approaches that primarily vary activator dosage, this study treats the alkali activator modulus (SiO 2 /Na 2 O molar ratio) as an independent chemical-control parameter. The effects of nominal modulus (0.6–1.4) and activator dosage (6%–10% relative to the total slag-fly ash precursor mass) on unconfined compressive strength, cohesion, and internal friction angle (φ) were systematically evaluated. X-ray diffraction and scanning electron microscopy were used to characterize phase-related and morphological changes and to support interpretation of the reaction mechanisms. The intermediate nominal modulus levels of 1.0 and 1.2 exhibited comparatively favorable mechanical performance, with M = 1.0 producing the highest values among the tested modulus levels. For the representative C = 8% specimens examined by SEM and XRD, M = 1.0 exhibited the most continuous and dense gel-like matrix among the three moduli investigated, consistent with more extensive reaction. At M = 1.0, the M10C10 mixture reached the peak 28-day unconfined compressive strength of 1.63 MPa, while the M10C8 mixture reached a 28-day cohesion of 499.11 kPa. At the lower modulus of M = 0.6, later-age strength regression and crystalline precipitation indicate an unfavorable low-modulus reaction environment; alkali migration and efflorescence-related processes are treated as possible contributing mechanisms rather than demonstrated causes. At M = 1.4, the lower effective alkalinity was associated with less extensive activation and lower strength. Considering the limited additional 28-day strength gain when the activator dosage increased from 8% to 10% at M = 1.0, M = 1.0 with an 8% dosage may be considered a dosage-efficient candidate when activator-use efficiency is prioritized over maximum short-term strength. The 28-day mechanical performance indicates potential for embankment and backfill applications, but long-term durability and environmental performance require further verification. These findings show that controlling activator modulus is important for tailoring the mechanical response and microstructure of slag-fly ash geopolymer-solidified dredged sludge.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Effect of Material Composition and Alkali Activator Modulus on Mechanical Properties and Reaction Process of Coal-Based Solid Waste Geopolymer.Materials (Basel, Switzerland) · 2026
- Effect of multi-source solid waste synergistic activation on strength evolution and micro-mechanism of dredged sludge stabilized with low-carbon curing agent.PloS one · 2026
- A review on the utilization of dredged sludge as a promising low-carbon supplementary cementitious material: activation, properties and microstructureJournal of Sustainable Cement-Based Materials · 2025
- Valorization of dredged sludge into sustainable subgrade materials through a novel industrial solid waste-derived stabilizer.Journal of environmental management · 2026
- Hydration Microstructure Three-Dimensional Modeling and Mechanical Performance of Slag-Based GeopolymersBuildings · 2026
- Synergistic Regulation Mechanism of Anti-Dispersion and Flowability of Alkali-Activated Slag Underwater Non-Dispersible Slurry.Materials (Basel, Switzerland) · 2026