Flexural-strength screening and acid-challenge response of bovine hydroxyapatite formulations with zirconia-based additions under formulation-specific sintering.
Lucas José de Azevedo-Silva, Brunna Mota Ferrairo, Lucas Yoshizawa de Marins, Marina Ciccone Giacomini, Paulo Noronha Lisboa-Filho, Ana Flávia Sanches Borges, Carlos Alberto Fortulan
Department of Prosthodontics and Periodontics, Faculty of Dentistry of Bauru, University of São Paulo, Bauru, Brazil. · Department of Operative Dentistry, Endodontics and Dental Materials, Faculty of Dentistry of Bauru, University of São Paulo, Bauru, Brazil.
Key points
From the paper's conclusion- Overall flexural-strength differences were significant ( p < 0.001).
Abstract
Hydroxyapatite-based (HA) bioceramics are attractive for dental-biomaterial development, but their mechanical and chemical limitations remain challenging. This study screened bovine-HA formulation-processing routes with zirconia-based additions by three-point flexural strength and then assessed chemical solubility, Vickers hardness, and qualitative surface morphology of the mechanically selected route after an acidic challenge. In Phase 1, pure HA and HA containing 1, 5, or 10 wt% 3Y-TZP or an exploratory nominal ZrO2 whisker-synthesis product were evaluated under formulation-specific sintering schedules. Overall flexural-strength differences were significant (p < 0.001). HA + 1 wt% 3Y-TZP showed the highest observed median [117.0 (94.8, 122.0) MPa], although its pairwise comparison with pure HA [84.0 (77.0, 88.0) MPa] did not reach significance (DSCF p = 0.095). In Phase 2, aggregate chemical solubility was 2,112.5 μg/cm2 for pure HA and 2,057.0 μg/cm2 for HA + 1 wt% 3Y-TZP; both exceeded the <2,000 μg/cm2 limit applicable to covered substructure ceramics in ISO 6872:2024 Classes 2-4, while monolithic ceramics are subject to the more stringent <100 μg/cm2 limit. HA + 1 wt% 3Y-TZP showed higher Vickers hardness than pure HA before (435.9 ± 26.4 vs. 217.0 ± 5.6 HV0.3) and after testing (426.9 ± 38.9 vs. 196.7 ± 10.5 HV0.3; Bonferroni-adjusted p < 0.001 for both). Pure HA showed a within-route decrease of -20.3 HV0.3 (95% CI: -33.1 to -7.5; adjusted p = 0.048), whereas the selected route showed a change of -9.0 HV0.3 (95% CI: -44.3 to 26.4; adjusted p = 1.000). Direct comparison of the changes was not significant (difference, -11.3 HV0.3; 95% CI: -46.7 to 24.1; adjusted p = 1.000), so differential hardness resistance to the acidic challenge was not demonstrated. Because composition and thermal history were not independently controlled, the findings should be interpreted as route-level screening rather than as an isolated zirconia effect or clinical validation.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Croaker Fish Bone-Derived Hydroxyapatite as a Sustainable Source for 3D-Printed Scaffolds for Bone Regeneration.Marine drugs · 2026
- Comprehensive Toxicological Evaluation of 3D-Printed Hydroxyapatite (3DPHA) for Bone Grafting ApplicationsInternational Journal of Molecular Sciences · 2026
- A comparative study on the characteristics of sintered hydroxyapatite derived from bovine bone powder, synthetic hydroxyapatite, and bovine hydroxyapatiteResults in Chemistry · 2026
- Advanced fabrication and characterization of robocasted halloysite-hydroxyapatite nanocomposite scaffolds for hard tissue regeneration.Frontiers in bioengineering and biotechnology · 2026
- Material-dependent effects of fish-scale-derived nano-hydroxyapatite on the mechanical, physicochemical, and optical properties of conventional glass ionomer cements.Clinical oral investigations · 2026
- New Na+,Mg2+,Zn2+ -containing hydroxyapatite/ZrO2 composites: preparation, mechanic properties and cytotoxicityBMC Chemistry · 2025