Degradation-structure-mechanical relationships of PLGA suture anchors and PCL coating-mediated mechanical preservation via degradation-induced crystallization.
Yao Lu, Jingbo Xu, Nan-Nan Li, Bing Hu, Songbiao Xue, Qingxia Song
College of Medical Devices, Zhejiang Pharmaceutical University, Ningbo, China. · Ningbo Weierkaidi Medical Devices Co., Ltd., Ningbo, China.
Key points
From the paper's conclusion- Here, we investigated the in vitro degradation of uncoated PLGA anchors over 24 weeks, structure-mechanical correlations through molecular weight-compression force coupling, and whether PCL coatings (5%, 10%, 20%) preserve mechanical performance through degradation-induced crystallization, complemented by a preliminary rat fascia-defect in vivo assessment.
Abstract
PLGA suture anchors are widely used for orthopedic soft-tissue fixation, yet their degradation-structure-mechanical evolution and the potential for coating-mediated mechanical regulation remain incompletely characterized. Here, we investigated the in vitro degradation of uncoated PLGA anchors over 24 weeks, structure-mechanical correlations through molecular weight-compression force coupling, and whether PCL coatings (5%, 10%, 20%) preserve mechanical performance through degradation-induced crystallization, complemented by a preliminary rat fascia-defect in vivo assessment. Uncoated anchors showed staged degradation: mass loss was modest through 8 weeks (<5.4%) but accelerated after 16 weeks (>35%), while Mn declined from ∼185,000 to ∼105,000 Da by 12 weeks and further thereafter. Compression Fmax remained at or above its initial value through 16 weeks despite ongoing chain scission, indicating structural-mechanical decoupling in which molecular degradation preceded macroscopic mechanical change. DSC confirmed that the material remained amorphous, with Tg remaining approximately 65 °C during degradation, and SEM revealed progressive surface pore formation. Among coated groups, PCL10% preserved mechanical performance best, with an initial ΔHm of about 46 J/g (Xc ≈ 33%) that increased further after 4 weeks, indicating a crystalline physical crosslink network; PCL5% degraded too rapidly and PCL20% showed no corresponding advantage. At Day 8 in vivo, blood and biochemical parameters showed individual deviations (n = 2 per group), and the implant caused notable local tissue reactions. Histology showed HE inflammatory cell density lower in sham (∼340-375 cells/mm2) than suture (∼743-813) and anchor (∼775-882), and CD206-positive densities remained below 10 cells/mm2 in all groups, with no inferential statistics. These findings define the structure-mechanical relationship governing PLGA anchor degradation and show that PCL10% coating preserves compression performance, providing a design rationale for absorbable anchor coatings, with boundaries set by the small in vivo sample, descriptive histology, batch differences, and single-point GPC data.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Thickness- and environment-dependent hydrolytic degradation of semi-crystalline poly(L-lactic acid) esophageal stents: a computational-experimental investigation.Journal of biomaterials science. Polymer edition · 2026
- Accelerating polycaprolactone degradation through bottlebrush architecture.Polymer chemistry · 2026
- Understanding Polycaprolactone Degradation: Molecular Mechanisms and Implications for Biomedical Device Design.Materials (Basel, Switzerland) · 2026
- Tuning the Printing Stability and Hydrolytic Degradation of Melt‐Electrowritten Poly(lactic‐co‐glycolic acid) Scaffolds Through Copolymer CompositionJournal of Polymer Science · 2026
- Stabilization of Electrospun Poly(lactide- co -glycolide) Meshes against Relaxation-Associated Bulk Shrinkage to Preserve Mesh ArchitectureACS Applied Polymer Materials · 2026
- Monolithic tissue sealant membrane with covalently‑anchored NHS‑activated gelatin adhesive moieties on flexible PLCL substrate: preparation, characterization and biological performance.Journal of biomaterials science. Polymer edition · 2026