◆ Journal of Advanced Ceramics2026-01-26· Materials science

Thickness-regulated interfacial polarization in CTAB-tailored Bi <sub>2</sub> WO <sub>6</sub> for enhanced piezocatalysis

Xiaoli Xu, Ying Wang, Wanwan Cheng, Huan Zhai, Jinqian Ma, Lingbo Xiao, Laishun Qin, Wenwen Liu, Yanmin Jia, Zhenhai Wen, Da Chen

原始摘要(英文原文)· Original abstract
While morphology regulation in conventional catalysis mainly increases the specific surface area to expose more active sites, in piezocatalysis it additionally alters the polarization properties of the materials. In this work, by leveraging the dual benefit of morphology regulation in piezocatalysis, we used cetyltrimethylammonium bromide (CTAB) to synthesize two-dimensional ultrathin Bi2WO6 (BWO) nanosheets, whose minimal thickness of ~ 2.26 nm results from the selective adsorption of CTAB inhibiting molecular layer stacking. This morphological control not only increase the specific surface area more than doubled from 14.47 to 29.15 m2 g‒1, but also enhance the interfacial polarization by 18.34 mV. Consequently, the effective piezoelectric coefficient of the CTAB-modified BWO rose from ~ 10.01 to ~ 27.53 pm V‒1. The modified catalyst, by simultaneously increasing reactive sites and boosting piezoelectric performance, achieves a maximum per-unit-power hydrogen production rate of 61.20 μmol g‒1 h‒1 W‒1, which is one of the highest values ever reported. This work demonstrates a synergistic strategy of morphology engineering to enhance surface reactivity and piezoelectric response, offering a new paradigm for high-performance piezocatalysts.
读原文 · Read the paper ↗

AI 追问PRO

登录后使用 AI 追问

讨论区

登录后参与讨论

相关论文 · Related

Thickness-regulated interfacial polarization in CTAB-tailored Bi <sub>2</sub> WO <sub>6</sub> for enhanced piezocatalysis — 科研速览 Science Skim