Paste volume fraction and aggregate fineness as design parameters for 3D-printed self-activated cementless mortars: buildability, compressive anisotropy, and flexural response
Jie Chen, Kinga Korniejenko, Chia-Ying Ho, Wei-Ting Lin
Key points
From the paper's conclusion- FM was the only factor that significantly affected flexural strength ( p = 0.008), and it was not correlated with compressive strength; the flexural–compressive coefficient averaged 0.84 for the finer and 1.09 for the coarser sand.
Abstract
Mix design for three-dimensional (3D)-printed mortars typically relies on the water-to-binder (w/b) and sand-to-binder (s/b) ratios, which become coupled when printability is held constant. This study examined whether the paste volume fraction ( V p ) and the aggregate fineness modulus (FM) can serve as practical design parameters for a self-activated ternary cementless mortar comprising ground granulated blast-furnace slag, co-fired fly ash, and fly ash, prepared without any external alkaline activator. Sixteen mixtures (s/b 1.00–1.75; FM 1.2 and 1.7; two binder compositions) were brought into a common printing window by a two-stage iso-workability procedure in which w/b and, where necessary, superplasticizer were adjusted as dependent variables. Stacking capacity ranged from 6 to 19 layers but was only weakly associated with mini-slump ( R 2 = 0.32) and unrelated to initial setting time ( R 2 = 0.04, p = 0.43). Only s/b was significantly associated with layer count ( R 2 = 0.36, p = 0.014), suggesting that the granular skeleton, rather than shape retention or setting kinetics, limited buildability. All mixtures exceeded 20 MPa at 56 days and reached about 70% of this strength within 7 days. V p described the 56-day axial compressive strength better than w/b and marginally better than s/b ( R 2 = 0.57, p < 0.001). Printed specimens matched mould-cast cubes in axial strength (mean ratio 0.98) but retained only 0.65 of it laterally; the anisotropy index (0.51–0.81) did not change with age and was not significantly affected by any design factor. FM was the only factor that significantly affected flexural strength ( p = 0.008), and it was not correlated with compressive strength; the flexural–compressive coefficient averaged 0.84 for the finer and 1.09 for the coarser sand. X-ray diffraction of the hardened pastes indicated consumption of the free lime and anhydrite supplied by the co-fired fly ash. Within the tested range, V p and FM acted mainly on different properties and can serve as complementary proportioning parameters, although the modest explained variance limits their predictive use.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Thermal Characterization of Low-Carbon Mortars Utilizing Multi-Source Fly Ash and Colloidal Nano-Silica for 3D Printing CompositesIOP Conference Series: Earth and Environmental Science · 2026
- Influence of Supplementary Cementitious Materials and Micro-Steel Fibers on 3D-Printed Concrete: Mechanical CharacterizationBuildings · 2026
- Printability assessment of concrete 3D printed elements with recycled fine aggregateConstruction and Building Materials · 2025
- Hardened Performance of 3D-Printed Geopolymer Mortars: A Review of Mechanical Properties, Durability, Sustainability, and Practical Implementation.Polymers · 2026
- One-Part vs. Two-Part Alkali-Activated GGBFS Mortars: Influence of Water-to-Binder Ratio on Extrusion-Based 3D Concrete PrintingInfrastructures · 2026
- New mix design for 3D printed mortar incorporating recycled fine aggregateDiscover Civil Engineering · 2026