Effects of high-translucent zirconia thickness and resin luting agent type on shear bond strength of zirconia restorations.
Keisuke Hoshino, Kei Kubochi, Hiroki Takata, Satomi Arai, Soichi Ikegami, Futoshi Komine
Department of Fixed Prosthodontics, Nihon University School of Dentistry, Tokyo, Japan.
Key points
From the paper's conclusion- Bonding performance was maintained when the thickness of high-translucent zirconia was ≤2.0 mm under standardized zirconia-to-zirconia bonding conditions. The effect of the type of resin luting agent varied depending on the zirconia thickness and polymerization conditions.
Abstract
PURPOSE: This study evaluated the effects of high-translucent zirconia thickness and resin luting agent type on shear bond strength (SBS). METHODS: In total, 352 high-translucent zirconia disks (diameter: 11.0 mm) with thicknesses of 1.0, 1.5, 2.0, and 2.5 mm were fabricated and bonded to 352 zirconia disks (diameter: 8.0 mm) using four resin luting conditions: dual polymerizing resin luting agent with 40 s of light-activated polymerization (UI40), direct composite resin with 40 s of light-activated polymerization (CM40), dual polymerizing resin luting agent without light-activated polymerization (UI0), and autopolymerizing resin luting agent (OP). Specimens were tested after 24 h in distilled water (TC0) or after 5,000 thermocycles (TC5,000). SBS, failure modes, and Knoop hardness were evaluated. RESULTS: At TC0, no significant differences in SBS were observed between the zirconia thicknesses in the UI40, CM40, and UI0 groups. At TC5,000, no significant differences were observed between the 1.0-, 1.5-, and 2.0-mm zirconia specimens in the UI40, CM40, and OP groups. UI40 and CM40 showed significantly higher SBS values than UI0 in the 1.0-, 1.5-, and 2.0-mm groups after TC5,000. However, OP did not differ significantly from UI40 and CM40 in the 2.0-mm group after TC5,000. Knoop hardness in the UI40 and CM40 groups was significantly lower in the 2.5-mm group than those at lower thicknesses. CONCLUSIONS: Bonding performance was maintained when the thickness of high-translucent zirconia was ≤2.0 mm under standardized zirconia-to-zirconia bonding conditions. The effect of the type of resin luting agent varied depending on the zirconia thickness and polymerization conditions.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Evaluation of Bond Strength of Different Surface-Treated Translucent Zirconia Blocks Luted with Universal Resin Cement to Glass-Reinforced Core Composite Before and After Aging: An In vitro Study.Journal of pharmacy & bioallied sciences · 2026
- Effect of Thermocycling and Surface Treatments on the Durability of Bond Strength of Translucent Zirconia to Resin Cement: An In Vitro Study.Cureus · 2026
- Influence of Zirconia Type and Surface Treatment on the Shear Bond Strength Between Veneering Porcelain and Zirconia.Dentistry journal · 2026
- Influence of surface treatment and simulated aging on the shear bond strength of different luting agents to zirconia.Dental and medical problems · 2026
- Optical properties of conventional and high-translucency zirconia ceramics and their effects on resin cement polymerization.Journal of dental sciences · 2026
- Adhesion performance of conventional and high-translucency zirconia: Effects of airborne-particle abrasion and 10-methacryloyloxydecyl dihydrogen phosphate treatments.Journal of dental sciences · 2026