Production of lightweight aggregate (LWA) by sintering blend of waste coal combustion ash (WCCA) and waste glass (WG): understanding the effect of WCCA chemical and mineralogical composition
Sharaniya Visvalingam, Noelle Lilan, Priscilla Kirabo, Jason B. Baxter, Yick G. Hsuan, Yaghoob Amir Farnam
Key points
From the paper's conclusion- The findings demonstrated that the suitability of WCCA for WCCA/WG-based LWAs production is strongly governed by WCCA melt-forming and iron oxide reduction potential, which is controlled by its chemical and mineralogical composition.
Abstract
This study investigated lightweight aggregates (LWAs) production using blends of waste coal combustion ash (WCCA) and soda-lime waste glass (WG), with a focus on understanding how the chemical and mineralogical composition of WCCA influences sintering behavior and LWA performance. LWAs were fabricated at a sintering temperature of 1100 °C using six types of WCCA with varying mass contents of Fe 2 O 3 , loss on ignition (LOI), amorphous phase, and mineral phases. The WG was used with contents ranging from 0 to 50 wt%. X-ray computed tomography (X-CT) and physical/mechanical testing showed that LWAs produced with 50% WG exhibited improved strength-to-specific gravity due to fewer large voids and higher solid integrity. However, at lower WG contents (25–40%), successful LWA formation was only achieved when the WCCA had favorable compositional traits, specifically, higher Fe 2 O 3 , LOI, amorphous content, and lower high-melting-point minerals such as mullite. These conditions promoted partial melting, enhanced gas generation, and facilitated iron oxide reduction during sintering, all of which were essential for producing structurally stable and well-bloated LWAs. On the other hand, dissolution and pH measurements revealed that WG contributed minimally to chemical activation of WCCA prior to sintering but acts as a binder during sintering. The findings demonstrated that the suitability of WCCA for WCCA/WG-based LWAs production is strongly governed by WCCA melt-forming and iron oxide reduction potential, which is controlled by its chemical and mineralogical composition. Understanding the effect of WCCA composition on sintering was found essential for optimizing WCCA/WG blend ratios and provide guidance for the future scale-up WCCA/WG-based LWAs production using WCCA and WG industrial byproducts.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Crystal-chemistry of phases in glass-ceramics prepared by reheating of municipal bottom ashes at different temperatures and duration times.Waste management (New York, N.Y.) · 2026
- Reinforcement methods and environmental assessment of sustainable cold-bonded artificial aggregates prepared from municipal solid waste incineration bottom ash.Environmental research · 2026
- Very-Low-Density Porous Aggregate Produced by Organomineral Surface Dusting with Kyzylorda TPP Ash and Ground Rice HuskConstruction Materials · 2026
- Sintering Behavior and Environmental Safety of Ceramsites Prepared from High-Alumina Fly Ash, Coal Gangue and Waste Glass.Materials (Basel, Switzerland) · 2026
- Valorization of kaolin waste via comparative calcination screening for alkali-activated binders in oil-well cementingJournal of Material Cycles and Waste Management · 2026
- Phase evolution and property development in kaolin ceramics based on soda lime silica and granite sludge wastesScientific Reports · 2025