Thermally induced moisture transport in concrete with different types of blended Portland cement studied by 1H-NMR relaxometry
Tim Pittrich, Simon Peters, Gunther Meschke, Frank Weise, Ludwig Stelzner
Federal Institute For Materials Research and Testing · Ruhr University Bochum
Key points
From the paper's conclusion- Therefore, thermally induced moisture transport in normal strength concretes made with different types of blended cements (CEM I, CEM II/A-LL, CEM III/A and CEM II/B-Q) was investigated by means of 1 H-NMR relaxometry in combination with supportive side investigations concerning permeability and porosity.
Abstract
Abstract Clinker-reduced cements are gaining in popularity as part of efforts to lower the construction industry’s CO 2 footprint. Past studies showed that utilization of these cements negatively influences the fire-induced spalling behavior of concrete, which is highly influenced by thermohydraulic damage mechanisms. Therefore, thermally induced moisture transport in normal strength concretes made with different types of blended cements (CEM I, CEM II/A-LL, CEM III/A and CEM II/B-Q) was investigated by means of 1 H-NMR relaxometry in combination with supportive side investigations concerning permeability and porosity. In addition, a numerical model was used to analyze in-situ moisture development during high temperature exposure. The results show that the cement type influences both initial moisture content and pore size-specific moisture distribution. This was primarily reflected in an increased water content in CEM III/A and CEM II/B-Q concretes as well as a comparable high gel pore water fraction in CEM II/B-Q concrete before heating. After heating, a similar degree of pore coarsening from gel to capillary pore was observed in all samples. Although the measurements were only conducted after, not during, high temperature exposure, the depth of the drying front and the extent of the moisture clog could be determined. With the additional numerical analysis, it can be assumed that during high temperature load, the drying front is less advanced and the moisture clog even more pronounced. In conclusion, it can be stated that the increased spalling susceptibility in blended cement concrete is caused by the lower initial permeability and increased moisture content.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Thermal decomposition in blended cement systems and its effect on fire-induced concrete spalling: Insights from XRD and TGACase Studies in Construction Materials · 2026
- Probe into the pore structure of carbonated calcium silicate cement compacts by proton nuclear magnetic resonance relaxometry.RSC advances · 2026
- A comparative study of OPC, WPC, and LC3 cements by low-field 1H TD NMRConstruction and Building Materials · 2025
- 4D imaging of microstructural evolution in alkali-activated slag cement pastes: linking pore-network topology to performanceCement and Concrete Composites · 2025
- Microstructural evolution of cement pastes under long-term carbonation: new insights in nanopores from water vapor sorption and 1H NMR relaxometryCement and Concrete Composites · 2025
- Wood biomass ash, municipal solid waste ash, and recycled concrete from construction demolition waste as supplementary cementitious materials in fine graded granular mixturesConstruction and Building Materials · 2025