Effect of Cleaning After Silica-Coating on the Resin Bond Strength to Zirconia.
Kétlin Fagundes Teixeira, Fernanda Cocco, Renatta Wrasse Temp, Gabriel Bauken, Pablo Machado Soares, Gabriel Kalil Rocha Pereira, Ana Carolina Cadore-Rodrigues, Luiz Felipe Valandro
Program in Oral Science, Faculty of Dentistry, Federal University of Santa Maria (UFSM), Santa Maria, RS, Brazil.
Key points
From the paper's conclusion- These findings indicate that cleaning protocol does not significantly affect zirconia-resin bond strength, and simpler approaches, such as air or air/water jets, are effective for maintaining bond strength after aging.
Abstract
This study assessed whether the cleaning protocol of the bonding surface of translucent zirconia, after silica-coating by air-abrasive particles, affects its resin bond strength before and after long-term aging. Zirconia slices (15×15×2 mm) (IPS e.max ZirCAD MT, Ivoclar) were air-abraded with silica-coated alumina particles, and then assigned to four cleaning protocol groups: air-jet only (AJ), air/water spray (AWS), ultrasonic bath with alcohol (UB-A), or ultrasonic bath with distilled water (UB-W). All surfaces received a primer (Monobond Plus, Ivoclar) followed by bonding the resin cement cylinders (Variolink Esthetic DC, Ivoclar; n=15), to be tested in microshear bond strength (µSBS) after 24 h of water storage (baseline) or after aging (90 days of water storage + 20,000 thermocycles, 5- 55 °C). Surface topography, elemental composition, and failure modes were also performed. Two-way ANOVA showed no significant effects of cleaning protocol (F=0.383, p=0.765), aging (F=3.196, p=0.077), or their interaction (F=0.443, p=0.723) on bond strength, although aged groups exhibited a higher incidence of pre-test failures. SEM revealed similar surface morphology among all groups, characteristic of silica-coated air abrasion. EDS detected residual silica in the AJ (0.8%) and AWS (0.13%) groups, whereas UB-A showed lower silica content (0.07%), and no silica was detected in UB-W. Despite these chemical differences, all cleaning protocols resulted in comparable bonding performance, with adhesive and cohesive failures observed across all groups. These findings indicate that cleaning protocol does not significantly affect zirconia-resin bond strength, and simpler approaches, such as air or air/water jets, are effective for maintaining bond strength after aging.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Effect of Thermocycling and Surface Treatments on the Durability of Bond Strength of Translucent Zirconia to Resin Cement: An In Vitro Study.Cureus · 2026
- Long-term enhancement of bond strength to zirconia using a modified tribochemical treatmentJournal of Adhesion Science and Technology · 2026
- Influence of Tooth Surface Pretreatment Procedure on Bond Strength of Self-Adhesive Cement-An In Vitro Study.Dentistry journal · 2026
- Which Bonding Protocol Provides the Most Durable Zirconia Adhesion after In Vitro Artificial Aging: A Systematic Review.The journal of contemporary dental practice · 2025
- Selective Infiltration Etching as a surface modification for high-translucency zirconia: Comparative analysis of roughness, composition, and bond strength.F1000Research · 2026
- Evaluation of Bond Strength of Different Surface-Treated Translucent Zirconia Blocks Luted with Universal Resin Cement to Glass-Reinforced Core Composite Before and After Aging: An In vitro Study.Journal of pharmacy & bioallied sciences · 2026