Effect of sub-Ac 3 normalizing temperature on microstructure and mechanical properties of deep-drawn low-carbon steel LPG cylinders
C. Sen Elkoca
Key points
From the paper's conclusion- Furthermore, while the correct normalizing temperature of 900 °C yielded a minimum average grain size of 5.54 µm, intercritical annealing at 800 °C led to significant surface grain coarsening to 14.16 µm due to decarburization.
Abstract
In this study, the reason for the decrease in mechanical test results after normalizing heat treatment in LPG cylinder manufacturing was investigated. To evaluate the effectiveness of the industrial heat treatment, deep-drawn steel sheet samples were annealed at temperatures ranging from 650 °C to 950 °C in a laboratory environment. Microstructural evaluations and hardness measurements revealed that improper industrial normalization temperatures led to heterogeneous grain structures and critical strength reductions. Specifically, annealing at the intercritical temperature of 800 °C caused severe subsurface decarburization, resulting in a sharp decrease in subsurface microhardness down to 89 HV10 compared to 193 HV10 of the core matrix. Furthermore, while the correct normalizing temperature of 900 °C yielded a minimum average grain size of 5.54 µm, intercritical annealing at 800 °C led to significant surface grain coarsening to 14.16 µm due to decarburization.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Phosphorus embrittlement in austenite during heat treatment of a medium-manganese steelEuropean Journal of Materials · 2026
- Effect of Sub-Zero Treatment on Microstructure, Retained Austenite, and Hardness of HSLA Steel for Automotive ApplicationsEvergreen · 2026
- The effect of cooling rate and calcium content on mechanical properties and the solidification characteristics of ZX magnesium alloys using cooling curve thermal analysisJournal of Materials Research and Technology · 2026
- Tempering Temperature‐Induced Microstructural Evolution and Corrosion Resistance of Laser Quenched 40CrNiMoA SteelMaterials and Corrosion · 2026
- The effect of heat treatment on microstructure and hardness of 9% Ni and 25% Mn cast steelsMATEC Web of Conferences · 2026
- Effect of tempering temperature on hydrogen embrittlement of X60 pipeline steelInternational Journal of Hydrogen Energy · 2025