Recovery of valuable metals from NMC811 lithium-ion cells and resynthesis via sol-gel process: a closed-loop hydrometallurgical approach

Tuğçe Selin Günşen, Meltem Yıldız

Key points

From the paper's conclusion
  • The originality of this work arises from the comparative study of chloride-, phosphate- and sulfamate-based leaching solutions for the recovery of metals and regeneration of the cathode material from waste NMC811 batteries.

Abstract

Studies were carried out to recover lithium, nickel, cobalt, and manganese from used, waste NMC811 lithium-ion cells by hydrometallurgical leaching using phosphoric, sulfamic, and hydrochloric acids. Where applicable, leaching efficiencies were determined based on measurements made by inductively coupled plasma optical emission spectroscopy (ICP-OES). The proportions of the various metal salts dissolved in the leachate required for the subsequent sol-gel synthesis reflect these efficiencies. As a result, hydrochloric acid yielded the highest total cathode recovery efficiency at 97.30 %, with individual metal recoveries of Li:99.45 %, Ni:98.08 %, Co: 97.41 %, and Mn:95.98 %. The total cathode with phosphoric acid recovery was found to be 96.29 %. The recovery efficiencies of the individual metals in the cathode were determined as follows: Li:81.70 %, Ni:80.28 %, Co:77.60 %, and Mn:74.91 %. According to the conducted study, the total cathode recovery with sulfamic acid was 95.43 %. The recovery efficiencies of the individual metals in the cathode were determined as follows: Li:75.98 %, Ni:67.51 %, Co:67.40 %, and Mn:63.61 %. The originality of this work arises from the comparative study of chloride-, phosphate- and sulfamate-based leaching solutions for the recovery of metals and regeneration of the cathode material from waste NMC811 batteries.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers