Abstract
The Fe3O4/SiO2 ratio is an important compositional factor affecting the mechanical behavior of magnetite ore like materials. In this study, uniaxial compression simulations were carried out using particle flow models with different Fe3O4/SiO2 ratios, and the simulated crack evolution and acoustic emission (AE) responses were interpreted together with SEM-EDS observations. The uniaxial compressive strength varies non monotonically with the Fe3O4/SiO2 ratio. As the ratio decreased from 3.00 to 1.00, the peak strength decreased from 131.64 MPa to 81.95 MPa. Further decreases in the ratio to 0.60 and 0.33 increased the peak strength to 146.45 MPa and 151.01 MPa, respectively. At Fe3O4/SiO2 = 1.00, the heterogeneous mineral interfaces appeared highly connected, and cracks preferentially initiated and coalesced along weak SiO2-Fe3O4 and Fe3O4-Al2O3 contacts, producing through going failure paths and the lowest strength. In SiO2 rich specimens, strongly bonded contacts formed a more stable load bearing framework that arrested or deflected cracks and improved strength. Crack number evolution and AE results show that failure was dominated by tensile crack propagation, whereas shear and mixed mode events were mainly associated with late stage coalescence, local sliding, and failure zone formation. SEM-EDS observations provide qualitative microstructural support for this mechanism: Si rich regions tend to impede crack propagation, whereas Si-Fe intergrown regions promote crack linkage. The strength variation is therefore attributed to ratio dependent changes in mineral contact combinations, the continuity of the load bearing framework, and the connectivity of heterogeneous interfaces.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Nanoscale fracture mechanisms in defective α‐ quartz induced by compression: Insights from molecular dynamics simulationDeep Underground Science and Engineering · 2026
- Finite Element Modeling of Selective Liberation of Copper Slag Under Impact CrushingRecycling · 2026
- Analysis of the Mechanism of Main Effects of Microscopic Parameters on Macroscopic Parameters in the PFC2D Parallel Bonding ModelApplied Sciences · 2026
- Inverse Analysis-Based Mesoscale Modeling and Microstructural Optimization of Silica Fume-Modified Asphalt ConcreteMaterials · 2026
- Influence of Grain-Scale Heterogeneity on Hydraulic Fracturing: A Study Based on a Hydro-Mechanical Phase-Field ModelMaterials · 2026
- Effects of Maximum Particle Size on the Shear Behavior of Coarse-Grained Soil: Direct Shear Tests and Discrete Element SimulationsEng · 2026