From the paper's conclusion
  • A micrometer-thick Frekote 770-NC film on P20 mold steel was treated using a 1064 nm nanosecond laser.

Abstract

Nanosecond laser cleaning of semi-permanent release-agent films requires balancing film removal and substrate modification. A micrometer-thick Frekote 770-NC film on P20 mold steel was treated using a 1064 nm nanosecond laser. Morphology, elemental composition, topography, wettability, and microhardness were evaluated. At 5-7 W, fluorine was below the detection limit of energy-dispersive X-ray spectroscopy. Local silicon contents were 0.46-0.68 wt.%, and relatively uniform scan-track overlap textures developed. The arithmetical mean height (S a ) was 0.615-0.670 µm, compared with 0.590 µm for bare P20. Mean Vickers microhardness peaked at 630.68 HV0.2 at 6 W, versus 310 HV0.2 for bare P20. Higher powers (9-12 W) produced texture coalescence and resolidified features. Under the tested single-pass conditions, treatment at 5-7 W reduced film coverage and yielded relatively regular surface textures, with accompanying surface hardening.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers

Power-dependent evolution of nanosecond laser removal of a semi-permanent release-agent film on P20 mold steel — Science Skim