Effect of adhesive primer on dentin mineral recovery by an alkasite compared to a glass hybrid restorative material: an in vitro study.
Yasmin Labib Nasr, Dina Mohamed Ali, Ahmed Fawzy Aboelezz
Conservative Dentistry Department, Faculty of Dentistry, Suez Canal University, Ismailia, Egypt. yamohammed@msa.edu.eg. · Conservative Dentistry Department, Faculty of Dentistry, Suez Canal University, Ismailia, Egypt.
Key points
From the paper's conclusion- The application of an adhesive primer significantly reduced the surface mineral recovery capacity of the alkasite material.
Abstract
BACKGROUND: Bioactive restorative materials can promote dentin mineral recovery, but their efficacy may be influenced by adhesive interfaces. This study aimed to evaluate the effect of an adhesive primer on the mineral recovery potential of an alkasite material (Cention Forte) compared to a glass hybrid material (Equia Forte HT) on artificially demineralized dentin. METHODS: Forty-two human molars with standardized Class V cavities were chemically demineralized and randomly divided into three restorative groups (n = 14): Cention Forte without primer (CF-P), Cention Forte with primer (CF + P), and Equia Forte HT (EF). After restoration, all samples underwent 14 days of pH cycling. Mineral recovery was evaluated using Vickers microhardness and energy-dispersive X-ray spectroscopy (EDX) at baseline (T0), after demineralization (T1), and after pH cycling (T2). RESULTS: All groups demonstrated significant longitudinal increases in absolute microhardness (p < 0.0001), following statistically comparable trajectories across materials (interaction, p = 0.748). Net microhardness recovery percentages were 74.21% ± 2.48% (CF-P), 72.50% ± 2.10% (EF), and 61.36% ± 3.22% (CF + P). In contrast, the elemental surface profile revealed material-specific differences in deposition with significant interactions (p < 0.01). Net calcium recovery was significantly lower in CF + P (68.91% ± 3.66%) than in CF-P (76.10% ± 5.58%) and EF (75.44% ± 2.85%; p < 0.05). Phosphorus recovery followed a matching pattern of primer-mediated attenuation (p < 0.05). The Ca/P ratio increased significantly in CF-P (p = 0.0005) and EF (p < 0.0001) but stalled in CF + P (p = 0.114). CONCLUSION: All restorative protocols achieved statistically comparable mechanical surface stabilization, though their underlying structural pathways diverged. The application of an adhesive primer significantly reduced the surface mineral recovery capacity of the alkasite material. Unprimed Cention Forte (CF-P) demonstrated comparable elemental deposition to the glass hybrid (EF), whereas primer application (CF + P) restricted localized ion-mediated precipitation.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Effects on adjacent enamel and dentin of restorations using bioactive materials under laboratory caries condition.American journal of dentistry · 2026
- Comparative Evaluation of the Mechanical Properties of an Alkasite-Based Material and a Conventional Resin Composite.Polymers · 2026
- Calcium/Phosphorus Ratio Changes in Demineralized Enamel and Dentin Adjacent to Ion-Releasing and Conventional Bulk-Fill Restorative Systems and Interfacial Micromorphology After Six Months in Artificial Saliva: An In Vitro SEM–EDX StudyDentistry Journal · 2026
- Adhesive Performance of Ion-Releasing Materials on Dentin with Altered Mineralization.Journal of functional biomaterials · 2026
- Clinical performance of alkasite and glass-hybrid restorations compared with resin composite in class II cavities: a randomized clinical trialClinical Oral Investigations · 2026
- The Remineralization Potential of Silver Diamine Fluoride, ReMin Pro, Bioactive Glass, and Grape Seed Extract on Artificial Enamel Lesions: An In Vitro Study.Biomimetics (Basel, Switzerland) · 2026