Evaluation of thermomechanical aging intervals associated with mechanical degradation of CAD/CAM materials in a chewing simulator.
Xiaojie Wang, Luiza Freitas Brum Souza, Moody Kaldas, Enkelejd Angelo Cankja, Tan Fırat Eyüboğlu, Mutlu Özcan
Center for Dental Medicine, Clinic of Masticatory Disorders and Dental Biomaterials, University of Zurich, Plattenstrasse 11, Zurich, CH-8032, Switzerland. · Center for Dental Medicine, Clinic of Masticatory Disorders and Dental Biomaterials, University of Zurich, Plattenstrasse 11, Zurich, CH-8032, Switzerland. mutluozcan@hotmail.com.
Key points
From the paper's conclusion- Lithium disilicate was the only material significantly impacted by aging, with the 600,000-cycle group showing the greatest observed reductions in flexural strength and reliability among the evaluated intervals. In contrast, Composite, LiSi, and Zirconia were not significantly affected, indicating greater resistance to thermomechanical fatigue.
Abstract
PURPOSE: To evaluate the influence of different thermomechanical aging intervals on the flexural strength and reliability of CAD/CAM restorative materials and to identify aging conditions that induce measurable mechanical degradation. METHODS: Specimens (N = 192) (16 × 4 × 2 mm3) were made from four CAD/CAM materials: resin-based composite (Brilliant Crios), lithium silicate ceramic (Initial LiSi Block), lithium disilicate ceramic (IPS e.max CAD), and monolithic zirconia (IPS e.max ZirCAD MT). Samples followed ISO 6872 (2015) for flexural strength testing and were divided into four aging groups (n = 12): baseline, 100,000, 600,000, and 1,200,000 cycles. Flexural strength was measured with a three-point bend test (1 mm/min, 12 mm span). Data were analyzed using ANOVA and Tukey's test (α = 0.05), and reliability was evaluated via Weibull analysis. RESULTS: Thermomechanical aging significantly reduced LD's flexural strength (p = 0.022), but not significantly for Composite (p = 0.141), LiSi (p = 0.158), or Zirconia (p = 0.064). The flexural strength of LD decreased by 23.1% after 600,000 cycles, while all materials showed their largest reduction then, but no significant differences were found among them. Weibull analysis showed a significant reliability drop in LD, with the lowest Weibull modulus after 600,000 cycles, while the reliability of others remained the same. CONCLUSIONS: Lithium disilicate was the only material significantly impacted by aging, with the 600,000-cycle group showing the greatest observed reductions in flexural strength and reliability among the evaluated intervals. In contrast, Composite, LiSi, and Zirconia were not significantly affected, indicating greater resistance to thermomechanical fatigue.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Impact of Thermocycling and Artificial Aging on the Flexural Strength and Fracture Resistance of CAD/CAM Dental Ceramics: A Systematic Review and Meta-Analysis.Dentistry journal · 2026
- Surface Treatment and Pre-Repair Thermal Aging Effects on Repair Bond Strength of Resin-Matrix CAD/CAM Ceramics.Biomimetics (Basel, Switzerland) · 2026
- Effects of thermocycling on color stability and mechanical properties of universal resin composites: an in vitro comparison.BMC oral health · 2026
- Effect of different finishing/polishing protocols and aging on flexural strength, roughness, and surface characteristics of definitive restorative materials for CAD/CAM.Clinical oral investigations · 2026
- Comparative evaluation of translucency changes in pre-shaded and externally stained CAD-CAM ceramics after thermocycling aging.Technology and health care : official journal of the European Society for Engineering and Medicine · 2026
- Deep Margin Elevation With Various Resin Composites: Effect of Thermomechanical Aging on the Marginal Gap of CAD / CAM InlaysJournal of Esthetic and Restorative Dentistry · 2026