Mechanical performance and color stability of 3D-printed ceramic-filled resin following various bleaching regimens: an in vitro study.
Tamer M Hamdy
Restorative and Dental Materials Department, Oral and Dental Research Institute, National Research Centre (NRC), Giza, Dokki, 12622, Egypt. tm.hamdy@nrc.sci.eg.
Key points
From the paper's conclusion- Home bleaching (16% carbamide peroxide) and in-office bleaching (40% hydrogen peroxide) reduced compressive and flexural strength, microhardness, and increased roughness of 3D-printed crowns. In-office bleaching showed greater effects, while color changes remained clinically acceptable.
Abstract
BACKGROUND: Recent material science advancements enabled a 3D-printable ceramic-filled resin for restorations. Additive manufacturing produces crowns, veneers, and mock-ups. Office and home bleaching agents contact teeth and restoration surfaces during application, potentially altering material properties. OBJECTIVES: The aim of the study is to assess the compressive strength, flexural strength, surface microhardness, surface roughness, and color changes of the additive 3D-printed ceramic-filled resin before and after exposure to home and in-office tooth bleaching. METHODS: A total of 150 specimens were equally distributed into control (non-bleaching), home-bleaching (16% carbamide peroxide), and in-office bleaching (40% hydrogen peroxide) groups (n = 50/group). Compressive strength was evaluated using a universal testing machine, flexural strength by a four-point bending test, surface microhardness using a Vickers hardness tester, surface roughness using a 3D optical profilometer, and color changes using a spectrophotometer based on the CIEDE2000 (ΔE00) system. Statistical analysis was performed using one-way ANOVA, Tukey post-hoc tests, and independent t-tests (α = 0.05). RESULTS: Both home bleaching (16% carbamide peroxide) and in-office bleaching (40% hydrogen peroxide) significantly reduced the compressive strength, flexural strength, and surface microhardness of the 3D-printed ceramic-filled resin while significantly increasing surface roughness (P ≤ 0.05). The in-office bleaching group exhibited significantly greater reductions in mechanical properties and higher surface roughness values than the home-bleaching group. Although bleaching produced statistically significant color changes, all ΔE00 values remained below the clinically acceptable threshold. CONCLUSIONS: Home bleaching (16% carbamide peroxide) and in-office bleaching (40% hydrogen peroxide) reduced compressive and flexural strength, microhardness, and increased roughness of 3D-printed crowns. In-office bleaching showed greater effects, while color changes remained clinically acceptable.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Influence of postprinting cleaning duration and glazing agents on the mechanical and surface properties of three-dimensionally printed dental resins: An in vitro study.The Journal of prosthetic dentistry · 2026
- Comparative Analysis of the Mechanical and Biofilm Surface Formation of 3D Printed Resins and Milled PMMA Blocks With and Without Inorganic Fillers.Clinical and experimental dental research · 2026
- Effect of post-print cleaning protocol on mechanical, optical, and conversion characteristics of two 3D-printed resin composites for definitive crowns.Journal of prosthodontics : official journal of the American College of Prosthodontists · 2026
- Surface Roughness of Direct, 3D-Printed and CAD/CAM Restorative Materials Following Different Bleaching ProtocolsApplied Sciences · 2026
- Effects of nitrogen-assisted post-curing and layer thickness on the properties of a 3D-printed ceramic-reinforced composite resin for permanent crowns under different aging conditions: an in vitro study.BMC oral health · 2026
- Erosive-Abrasive Effects on Surface, Mechanical, and Optical Properties of 3D-Printed Resin Composites for Prosthetic Applications.The International journal of prosthodontics · 2026