Effects of high temperature with pressure polymerization on the physical and mechanical properties and dimensional changes of 3D-printed denture teeth resin
Shanglin Wu, Yuriko Komagamine, Tamaki Hada, Keyu Qi, Pong Pongprueksa, Manabu Kanazawa
Tokyo Medical and Dental University · Mahidol University
Key points
From the paper's conclusion- Therefore, this study aimed to analyze the impact of high temperature with pressure polymerization on the degree of conversion, Vickers hardness, flexural strength and modulus, and dimensional changes of 3D-printed denture teeth resin.
Abstract
BACKGROUND: The optimal post-treatment methods for improving the mechanical properties and degree of conversion of three-dimensional (3D)-printed denture teeth resin remain unclear. Therefore, this study aimed to analyze the impact of high temperature with pressure polymerization on the degree of conversion, Vickers hardness, flexural strength and modulus, and dimensional changes of 3D-printed denture teeth resin. METHODS: In total, 180 specimens (Dima Print Denture Teeth A3; Kulzer) fabricated from the denture teeth resin using a digital light processing 3D printer (Cara printer 4.0; Kulzer) were randomly divided into five groups: no post-treatment (control) and post-treatment at 121 °C for 4, 30, 60, or 90 min. The air pressure applied during the treatments was set at 2 bar and was maintained throughout the post-polymerization process. Furthermore, 30 rectangular-shaped specimens (22 × 4 × 2 mm) were used for the degree of conversion test (6 specimens/group), 50 disk-shaped specimens (10 mm diameter × 2 mm thickness) were used for the Vickers hardness test (10 specimens/group), and 50 bar-shaped specimens (25 × 2 × 2 mm) each were used for the flexural strength, flexural modulus, and dimensional change tests (10 specimens/group). The degree of conversion, flexural modulus, and dimensional change of width were analyzed by one-way analysis of variance (ANOVA), followed by Tukey's honest significant difference post hoc test. The flexural strength, Vickers hardness, and dimensional change of length were analyzed by Welch's ANOVA, followed by Dunnett's T3 multiple comparisons post hoc tests. The dimensional change of thickness was analyzed with a Kruskal-Wallis analysis and a post hoc comparison using the Mann-Whitney U test (α = 0.05). RESULTS: The degree of conversion and Vickers hardness values were the lowest in the control group and the highest in the 121 °C/90 min group. The flexural properties and error rates for length, width, and thickness were also the highest in the 121 °C/90 min group. CONCLUSIONS: Post-treatment at 121 °C for 90 min increases the degree of conversion and surface hardness of 3D-printed denture teeth resin, without damaging the resin's flexural properties, and maintains dimensional changes within acceptable limits.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Enhancing Wear Resistance and Surface Hardness of Three-Dimensionally Printed Denture Teeth Through Post-Treatment Under Elevated Temperature and Pressure.Journal of functional biomaterials · 2026
- Effect of printing temperature on the viscosity, photopolymerization, and mechanical properties of a highly filled 3D-printing dental resin composite.Journal of the mechanical behavior of biomedical materials · 2026
- Heat-assisted vat-polymerization and light irradiance impact on 3D-printed dental resin composites.Journal of the mechanical behavior of biomedical materials · 2026
- Effect of Printing Orientation and Post-Curing Time on the Mechanical Properties of 3D-Printed Denture Base ResinJournal of Functional Biomaterials · 2025
- Influence of 3D-Printing system on the mechanical and surface properties of a 3D-Printed denture base resin.Journal of applied biomaterials & functional materials · 2026
- Flexural strength and flexural modulus of repaired 3D-printed denture base resin: Effects of reinforcement and thermal cycling.Journal of prosthodontic research · 2026