International Journal of Polymer Science

Effect of Harvest Location and Fiber Extraction Zone in the Stem Bark of Abelmoschus esculentus on Its Chemical, Physical, and Mechanical Properties

Jonas Peequeur Essome Mbang, Anne-Marie Ndzie Bidima, Suzie Viviane Obame, Michel Mbere Taoga, Crépin Constant Joueyon Ngok, Frank Loïc Gnintedem Zebaze, Pierre Marcel Anicet Noah, Fabien Betene Ebanda

Key points

From the paper's conclusion
  • These findings demonstrate that the sampling zone is the key parameter controlling fiber quality and highlight the strong potential of okra stem bark fibers for sustainable textile products and bio‐based composite applications.

Abstract

In response to the growing demand for sustainable materials derived from renewable resources, this study investigated the influence of harvest location (Littoral and West regions of Cameroon) and fiber extraction zone (bottom, middle, and top of the stem) on the properties of Abelmoschus esculentus (okra) stem bark fibers. The fibers were extracted through biological retting and characterized using Fourier transform infrared spectroscopy coupled with attenuated total reflectance (FTIR‐ATR), chemical analyses, physical tests, scanning electron microscopy (SEM), and tensile mechanical testing. FTIR‐ATR spectra confirmed the lignocellulosic nature of the fibers through the presence of hydroxyl (O–H), aliphatic (C–H), carbonyl (C=O), aromatic lignin (C=C), and β ‐glycosidic cellulose functional groups. Chemical analysis revealed cellulose, hemicellulose, lignin, and pectin contents ranging between 60.98% and 68.30%, 13.05% and 16.45%, 7.15% and 10.10%, and 8.55% and 16.41%, respectively, with the highest cellulose content observed in fibers extracted from the middle stem section. Physical characterization showed linear density values of 10.00–12.22 tex, water absorption capacities of 105%–160%, densities of 0.95–1.21 g/cm 3 , and water contents of 11.39%–12.73%. SEM observations revealed that middle‐section fibers exhibited a more compact and less porous structure than fibers from the bottom and top sections. Mechanical testing indicated a brittle behavior, with tensile strength ranging from 102.0 to 170.9 MPa, Young′s modulus from 3.3 to 5.1 GPa, tenacity from 19.21 to 33.25 cN/tex, initial modulus from 988 to 1450 cN/tex, and elongation at break below 5%. Overall, fibers extracted from the middle section displayed the most homogeneous properties and the best mechanical performance, regardless of harvest location. These findings demonstrate that the sampling zone is the key parameter controlling fiber quality and highlight the strong potential of okra stem bark fibers for sustainable textile products and bio‐based composite applications.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers