Advances in Materials Science and Engineering

Investigating the Effect of TiO 2 on the Physical and Mechanical Properties of Roller‐Compacted Concrete Pavement Containing Ground Granulated Blast‐Furnace Slag Using Response Surface Methodology

Abbas Maniseresht

Key points

From the paper's conclusion
  • This study investigates the effects of replacing ordinary Portland cement (OPC) with titanium dioxide (TiO 2 ) at replacement levels of 0%, 5%, and 10%, in conjunction with ground granulated blast‐furnace slag (GGBS) at 0%, 30%, and 60%, on the physical and mechanical properties of roller‐compacted concrete (RCC) pavement fabricated via the soil compaction method.

Abstract

This study investigates the effects of replacing ordinary Portland cement (OPC) with titanium dioxide (TiO 2 ) at replacement levels of 0%, 5%, and 10%, in conjunction with ground granulated blast‐furnace slag (GGBS) at 0%, 30%, and 60%, on the physical and mechanical properties of roller‐compacted concrete (RCC) pavement fabricated via the soil compaction method. Response surface methodology (RSM) was employed to develop predictive models and optimize compressive strength at 28 and 90 days, as well as flexural strength, splitting tensile strength, and water absorption at 90 days of curing. The experimental results indicate that the addition of TiO 2 alone increased compressive, flexural, and splitting tensile strengths while reducing porosity and water absorption, with optimal performance at a 10% replacement level. Conversely, the individual incorporation of GGBS reduced 28‐day compressive strength. By 90 days of curing, however, a 30% GGBS replacement significantly improved all mechanical strength metrics, while the 60% GGBS mix yielded the lowest overall porosity and water absorption. When binary modifiers (TiO 2 and GGBS) were combined, early‐age (28‐day) strengths declined. Nonetheless, by Day 90, a blend containing 5% TiO 2 and 30% GGBS showed a marginal increase in strength. Notably, the incorporation of TiO 2 and GGBS—both individually and in combination—consistently lowered porosity and water absorption across all cohorts, with the 10% TiO 2 and 30% GGBS blend exhibiting the lowest values. Multiobjective RSM optimization for a 90‐day curing regime revealed three optimal configurations: (1) TiO 2 ‐only: 10% replacement maximizes strength and minimizes porosity. (2) GGBS‐only: Optimal performance peaks at a 39.3% threshold. (3) Binary system: The model predicted an optimum at 10% TiO 2 paired with just 2.02% GGBS. These RSM‐optimized formulations strongly agree with the empirical laboratory data. SEM analysis confirmed that both individual and blended applications of GGBS and TiO 2 refine the RCC matrix microstructure. The modifiers promote uniform particle distribution, effectively densify interstitial voids, and significantly reduce porosity compared to the unmodified control specimens. “A preprint has previously been published Maniseresht, A., 2025.”

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.