Crack‐Tip Stress Distribution and Fractographic Analysis of Brittle Fracture in AA7075‐T6 Aluminium Alloy
Tryphone Obuya Oloo, Oludolapo Akanni Olanrewaju, Samson Oluropo Adeosun
Key points
From the paper's conclusion- The overload fracture surface was flat and faceted with few large dimples, consistent with the low ductility of the T6 temper; higher‐resolution fractography and metallographic sectioning are identified as necessary to establish the fracture micromechanism.
Abstract
Understanding how stresses are distributed around crack tips in high‐strength aluminium alloys is essential for predicting fracture initiation sites, crack deflection and the transition from stable cracking to unstable fracture. This paper analyses the Mode I crack‐tip stress field in fatigue pre‐cracked single‐edge‐notched tension (SENT) specimens of AA7075‐T6 (L‐T orientation) using the singular term of Williams’ asymptotic solution in Cartesian and polar coordinates, a two‐dimensional finite element (FE) model in Ansys Mechanical APDL 2026 R1, and scanning electron microscopy (SEM) with quantitative image analysis. At the maximum test load, the stress intensity factor was K I = 13.08 MPa√m ( a 0 = 3.5 mm, σ = 94.85 MPa), giving a conditional fracture toughness K Q = 13.1 ± 0.2 MPa√m for the three specimens. The FE model, built with a symmetric spider‐web mesh and quarter‐point crack‐tip elements, converged to within 0.2% of this value. The plane‐stress plastic zone extends 0.11 mm ahead of the crack ( r p / W ≈0.5%), so small‐scale yielding applies, and the ASTM E399 size requirement of 1.70 mm is met; the toughness nevertheless remains conditional because the 5% secant‐offset load could not be evaluated. The FE and Williams opening stresses agree to within 3% at 0.3 mm ahead of the tip, but differ by 10%–31% between 1 and 3 mm, which limits the K‐dominated zone in this geometry to about 0.1a. SEM of the untested surface revealed elongated cavities up to 77 μm long and pits of about 670 μm 2 , interpreted as sites of torn‐out coarse constituent particles that can act as crack initiation sites. The overload fracture surface was flat and faceted with few large dimples, consistent with the low ductility of the T6 temper; higher‐resolution fractography and metallographic sectioning are identified as necessary to establish the fracture micromechanism.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Influence of T6 Heat Treatment on Distortion-Relevant Cutting Forces and Surface Residual Stresses in Orthogonal Cutting of Aluminium Casting Alloy AlSi7Mg0.3Journal of Manufacturing and Materials Processing · 2026
- Predicting the Size‐Dependent Fatigue Strength Distributions in Additively Manufactured AlSi10Mg Alloy Specimens Using Extreme Value StatisticsFatigue & Fracture of Engineering Materials & Structures · 2026
- Anisotropic fatigue limit estimation for a notched single crystal superalloy based on the theory of critical distancesInternational Journal of Fatigue · 2025
- A High-Temperature Semi-Coupled Damage Model for 7075 Aluminum Alloy Considering Temperature and Strain Rate Effects.Materials (Basel, Switzerland) · 2026
- Numerical investigation of residual stress influence on fatigue crack propagation in orthotropic steel bridge decks under traffic loadsEngineering Fracture Mechanics · 2026
- Fatigue assessment of 316L DED-arc structures considering individual surface topographyWelding in the World · 2026