Structure–Property–Durability Relationships of BaSO 4 ‐Filled Polyurea Elastomer Coatings Optimized by Response Surface Methodology

Xuan Thang Dam, Thi Thanh Luong, Thuy Van Ngo, Minh Thanh Do

Key points

From the paper's conclusion
  • These results establish a validated formulation–processing–durability framework for BaSO 4 ‐filled PUa coatings for concrete protection.

Abstract

Polyurea (PUa) elastomer coatings are promising for concrete protection, but balancing mechanical performance, adhesion, processing quality, and environmental durability remains challenging. Here, barium sulfate (BaSO 4 )‐filled PUa coatings were optimized using a three‐factor Box–Behnken design (BBD) involving BaSO 4 content, A/B mass ratio, and vacuum level. Quadratic response‐surface models showed strong predictive quality ( R 2 = 0.9938–0.9977). Pareto‐based multiresponse optimization identified PUa.20–0.75–12.5 (20 wt% BaSO 4 , A/B = 0.75, −12.5 inch Hg) as the minimum‐distance‐to‐utopia compromise condition. Validation yielded a tensile strength of 20.34 ± 0.63 MPa, elongation at break of 1067.21% ± 11.72%, and pull‐off adhesion of 3.96 ± 0.08 MPa, with prediction errors below 2%. Fourier transform infrared (FTIR) and scanning electron microscopy (SEM) supported urea‐rich network formation, predominantly physical BaSO 4 incorporation, improved filler dispersion, and suppression of void‐related defects, while differential scanning calorimetry (DSC) and dynamic mechanical thermal analysis (DMTA) revealed formulation‐ and environment‐dependent thermal and viscoelastic responses. Environmental durability was quantified using normalized retention ratios, apparent decay constants ( k env ), and a study‐specific environmental aggressiveness index (EAI). Among the environments included in the quantitative retention analysis, apparent aggressiveness followed alkaline water > dry storage at 5°C > neutral water, with EAI values of 0.0580, 0.0341, and 0.0088 month −1 , respectively. Xylene exposure was assessed separately through SEM, gel‐fraction, and swelling analyses. These results establish a validated formulation–processing–durability framework for BaSO 4 ‐filled PUa coatings for concrete protection.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers