Durability of PVA Fiber Reinforced Concrete Under Combined Salt Freeze–Thaw and Dry–Wet Cycles
Binbin Wan, Chaoyong Wang, Qiuyue Wang, Dengfeng Qiu, Dake Wu
Key points
From the paper's conclusion- Using freeze–thaw in fresh water and plain concrete as controls, the durability of concrete with three fiber volume contents (0.2%, 0.3%, and 0.4%) at the same fiber length of 12 mm under coupled salt freeze–thaw and dry–wet cycling conditions was investigated.
Abstract
Concrete in cold saline regions is prone to damage such as surface spalling, pore expansion, and strength degradation due to long‐term salt freeze–thaw attack. The use of polyvinyl alcohol (PVA) fiber to improve its performance has application potential, but the modification effect of fiber content under coupled salt freeze–thaw and dry–wet cycling conditions needs to be systematically clarified. In the experiment, a C40 concrete mix proportion with a water‐to‐binder ratio of 0.45 and a sand ratio of 0.4 was selected. Using freeze–thaw in fresh water and plain concrete as controls, the durability of concrete with three fiber volume contents (0.2%, 0.3%, and 0.4%) at the same fiber length of 12 mm under coupled salt freeze–thaw and dry–wet cycling conditions was investigated. The evolution of performance was clarified through changes in mass, compressive strength, and water absorption, as well as microstructural analysis. The test results revealed a two‐stage evolution of concrete performance. In the early erosion stage, the concrete was in a densification enhancement stage, during which the strength showed an upward trend and the water absorption decreased. In this stage, the compressive strength of the 0.3% fiber content group at 14 days increased by 21.5% compared with plain concrete, showing the best improvement effect. In the middle and late stages, the concrete entered a deterioration stage, during which the mass fluctuated and the strength decreased. The deterioration of plain concrete was the most obvious; at 56 days, its compressive strength decreased by 31.6% compared with the peak value, and the apparent damage was relatively more severe. At the micro level, in the initial stage of erosion, salt compounds react to form gypsum and ettringite, which fill the pores. In the later stage, however, the expansion of gypsum leads to an increase in porosity and a looser structure. Among the fiber contents investigated in this study, 0.3% provided the best overall performance.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Degradation mechanism and compressive strength prediction of polyvinyl alcohol fiber-engineered cementitious composites under coupled salt corrosion and freeze-thaw cyclesConstruction and Building Materials · 2025
- Freeze-Thaw Damage Evolution of PVA-Fly Ash-Slag Composite Concrete and Low-Dimensional Mapping of Weibull Characteristic Parameters.Materials (Basel, Switzerland) · 2026
- Influence of Fly Ash-Ground Granulated Blast Furnace Slag Blends and PVA Fibres on the Dimensional Stability, Durability and Microstructure of Foamed Concrete.Materials (Basel, Switzerland) · 2026
- A comprehensive review on the performance, mechanisms and design of polyvinyl alcohol (PVA)-enabled self-healing concreteJournal of Building Engineering · 2026
- A study on drying shrinkage properties of PVA fiber reinforced coal gangue fine aggregate concreteResults in Engineering · 2026
- Sulfate resistance of polyvinyl alcohol and basalt fibers reinforced red mud concrete.PloS one · 2026