Effects of Build and Support Configuration on the Flexural Strength and Fatigue Behavior of LCM‐Printed Alumina
Augusto Botton Pozzebon, Dalton Daniel de Lima, Kétlin Fagundes Teixeira, Gabriel Kalil Rocha Pereira, Luiz Felipe Valandro, Natália de Freitas Daudt
Key points
From the paper's conclusion- These results indicate that build orientation and support configuration, not densification alone, influence the mechanical reliability of LCM‐printed alumina, and that support‐related differences may become evident only under cyclic loading.
Abstract
Lithography‐based ceramic manufacturing (LCM) produces complex alumina components with high accuracy; however, its layer‐by‐layer construction introduces anisotropy that remains insufficiently characterized. This study evaluated the effects of build orientation and support configuration on the mechanical performance of LCM‐printed alumina. Unsupported bars printed in three orientations ( X , Y , Z ) were assessed for linear shrinkage, Vickers hardness, and three‐point flexural strength, including Weibull analysis. Discs printed on the build platform (CM), on vertical (CSV) and horizontal (CSH) supports were tested under monotonic and step‐stress cyclic loading in the piston‐on‐three‐balls configuration (ISO 6872:2024). High relative densities (96.6%–98.3%) were achieved under all conditions. Characteristic flexural strength depended strongly on build orientation, increasing from 219 MPa in Z to 351 MPa in X and 403 MPa in Y (a 46% reduction from Y to Z ), while Weibull moduli could not be statistically distinguished. Under monotonic loading, no statistically significant effect of support configuration was detected with the present sample size ( n = 5 per group; F (2,12) = 3.73, p = 0.055). In contrast, under cyclic loading, the mean failure stresses of CSV (255 MPa) and CSH (187 MPa) were 29.3% and 48.1% below their monotonic characteristic strengths, whereas no degradation was detectable for CM (295 MPa) within the resolution of the step‐stress protocol. Fracture originated at tensile‐surface defects in all disc groups. These results indicate that build orientation and support configuration, not densification alone, influence the mechanical reliability of LCM‐printed alumina, and that support‐related differences may become evident only under cyclic loading.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Toward Predictive Dimensional Accuracy in DLP-Fabricated Alumina Lattices: Volumetric Error and Shrinkage ControlACS Omega · 2026
- Experimental investigation of build orientation effects on mechanical and fracture behaviors of additively manufactured lattice materialsMechanics of Advanced Materials and Structures · 2026
- UV-Based In Situ Photocuring-Assisted Direct Ink Writing of Unsupported Multi-Scale and Large-Span Alumina PreceramicCoatings · 2026
- Effects of build orientation and manufacturing system characteristics in digital light processing additive manufacturing on the properties of zirconia.Journal of the mechanical behavior of biomedical materials · 2026
- Tribological performance of stereolithography processed alumina: orientation effects and wear mechanismsJournal of Materials Research and Technology · 2026