Interface Optimization for Balanced Fiber Protection and Matrix Densification in SLA‐Printed Cf/SiC With Fine Pores
Qiming Chen, Lei Qiao, Yuekai Yan, Junyang Zhou, Chuanqi Hu, Shan Li, Gong Wang, Hui Mei,
Key points
From the paper's conclusion- This work demonstrates that for SLA‐printed green bodies with fine pore‐channel structures, coordinated fiber protection and pore‐channel regulation are essential for fabricating high‐performance C f /SiC composites.
Abstract
SLA‐printed C f /SiC green bodies usually contain fine and tortuous pore channels, which makes it difficult to simultaneously construct fiber protective layers and achieve sufficient densification. To overcome this challenge, PyC interlayers and SiC protective layers were successively fabricated on exposed carbon fiber surfaces by chemical vapor infiltration (CVI) or precursor infiltration and pyrolysis (PIP), forming PIP–PyC/PIP–SiC (PyC l ‐SiC l ), CVI–PyC/CVI–SiC (PyC g ‐SiC g ), and CVI–PyC/PIP–SiC (PyC g ‐SiC l ). The effects of these PyC/SiC protective layers on pore‐channel regulation, mechanical properties, and fiber protection were systematically investigated. CVI–PyC provided more continuous fiber encapsulation than PIP–PyC, while PIP–SiC preserved pore connectivity more effectively than CVI–SiC. The PyC l ‐SiC l layer retained relatively complete pore channels, but its insufficient fiber protection during densification process led to poor mechanical properties. The PyC g ‐SiC g layer protected fibers effectively; however, pore blockage restricted densification and weakened its mechanical performance. In contrast, the PyC g ‐SiC l configuration achieved the best balance between fiber protection and infiltration‐channel retention, enabling sufficient densification. Its flexural strength and fracture toughness reached 263.98 ± 8.34 MPa and 4.00 ± 0.27 MPa·m 1/2 . This work demonstrates that for SLA‐printed green bodies with fine pore‐channel structures, coordinated fiber protection and pore‐channel regulation are essential for fabricating high‐performance C f /SiC composites.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Slurry Carbon–Driven Pore Evolution, Infiltration, and Mechanical Properties of Continuous Carbon Fiber‐Reinforced Silicon Carbide Composites Prepared by Slurry Impregnation Combined With Reaction Melt InfiltrationJournal of the American Ceramic Society · 2026
- Infiltration Behavior and Pore Evolution of C f /SiC Composites Prepared by SI–RMI: Influence of Slurry Solid LoadingJournal of the American Ceramic Society · 2026
- Ultrasonic vibration-assisted nanoscale cutting of SiC fiber sidewalls in SiCf/SiC composites with a PyC interphase: A molecular dynamics study of interphase thickness effectsEngineering Research Express · 2026
- Enhanced Strength of Porous YSZ Ceramics via Slurry Infiltration Into Semi‐Sintered BodiesInternational Journal of Applied Ceramic Technology · 2026
- Effects of carbothermal reduction on microstructure and mechanical properties of PIP-based Cf/SiOC compositesJournal of the Korean Ceramic Society · 2025
- Ceramic Slurry Design for Vat‐Photopolymerization of Turbine Blade Ceramic Cores: A ReviewJournal of the American Ceramic Society · 2026