Journal of the American Ceramic Society

Sulfuric Acid Degradation of Alkali‐Activated Fly Ash–Slag Binders: Multiscale Evolution and Paradoxical Role of Ca

Shengqian Ruan, Jian‐Xin Lu, Wenlin Tu, Dingqiang Fan, Xudong Zhao, Hao Qian, Chi Sun Poon

Key points

From the paper's conclusion
  • These findings distinguish resistance to acid ingress from the preservation of residual‐skeleton integrity and provide new insights into degradation modes, gel‐skeleton evolution, and composition‐informed design of AAFS binders.

Abstract

Alkali‐activated fly ash–slag (AAFS) binders have attracted interest as alternative cementitious materials for applications exposed to sulfuric acid, for example, in sewer environments. However, how binder chemistry governs degradation behavior and resistance remains insufficiently understood, particularly regarding structural evolution and damage mechanisms. This study investigated AAFS binders with different precursor compositions (slag content: 10%–75%) and activator chemistries (dosage: 15% and 20%; Ms: 1 and 2) under sulfuric acid exposure, with weekly solution renewal at an initial pH of 1.0 (rising to 1.5–1.9 before renewal). Decreasing slag content generally reduced the 90‐day compressive strength before exposure. Higher activator dosage and Ms also resulted in slight reductions in strength. After a 90‐day exposure, the spatially continuous evolution of the residual gel skeleton across the degraded zone was tracked using multiscale imaging techniques and microhardness testing. The results revealed a paradoxical role of Ca. High‐Ca, slag‐rich AAFS formed denser matrices with greater acid–neutralization capacity, resulting in a 90‐day degradation depth up to 64.8% lower than that of low‐Ca AAFS. However, high‐Ca AAFS developed network cracking and a spalling‐prone weak layer due to decalcification, dealumination, and gypsum‐induced stress, retaining only 15.0%–29.7% of the unaffected‐matrix microhardness. In contrast, low‐Ca AAFS showed faster acid penetration but retained a more continuous, Al‐rich skeleton, with 36.4%–53.3% microhardness retention. These findings distinguish resistance to acid ingress from the preservation of residual‐skeleton integrity and provide new insights into degradation modes, gel‐skeleton evolution, and composition‐informed design of AAFS binders.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers

Sulfuric Acid Degradation of Alkali‐Activated Fly Ash–Slag Binders: Multiscale Evolution and Paradoxical Role of Ca — Science Skim