Journal of the American Ceramic Society

Effect of Boron Source on Microstructure and Mechanical Properties of SiBCN Ceramics

Peng Qi, Donghua Xu, Litao Yin, Hanzhao Tian, Yan Wang, Qian Zhang, Zibo Niu, Daxin Li,

Key points

From the paper's conclusion
  • SiBCN‐2 exhibits enhanced sintering activity, and its mechanical properties rapidly improve at 1900°C, with flexural strength and fracture toughness reaching 202.3 MPa and 6.34 MPa·m 1/2 , respectively.

Abstract

Mechanically alloyed amorphous SiBCN powders with two different boron sources ( h ‐BN and elemental B) were hot‐pressed at 1800°C, 1900°C, and 2000°C under a pressure of 50 MPa in nitrogen atmosphere for 30 min. The phase transformation, microstructural evolution, and mechanical properties of the prepared ceramics were systematically investigated by XRD, TEM, SEM, and mechanical testing. Results show that the precipitation of β‐Si 3 N 4 , β‐SiC, and BN(C) in the amorphous matrix strongly depends on the reactivity of boron precursors. The SiBCN‐1 derived from h ‐BN precursor forms β‐Si 3 N 4 , β‐SiC, and lamellar BN(C), and achieves a maximum flexural strength of 60.2 MPa at 2000°C. SiBCN‐2 exhibits enhanced sintering activity, and its mechanical properties rapidly improve at 1900°C, with flexural strength and fracture toughness reaching 202.3 MPa and 6.34 MPa·m 1/2 , respectively. However, oversintering at 2000°C induces severe BN‐rich segregation and obvious degradation in mechanical performance.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers

Effect of Boron Source on Microstructure and Mechanical Properties of SiBCN Ceramics — Science Skim