Mechanical Properties of High‐Purity, High‐Density NaSICON (Na 1+ x Zr 2 Si x P 3− x O 12 , 2 ≤ x ≤ 2.8)
Seneca Stevens, Tanmay Mohan Bhagwat, Hannah Howard, Zhengwu Fang, Cathy Wang, Egan MacLeod, Miaofang Chi, Daniel S. Gianola,
Key points
From the paper's conclusion- Here, we report the first comprehensive mechanical characterization of high‐purity (total secondary‐phase content < 10%), fully dense NZSP across x = 2.0–2.8, prepared by rapid induction hot‐pressing of powders prepared by solution‐assisted solid‐state reaction.
Abstract
NaSICON (Na Super Ionic Conductor) ceramics with formula Na 1+ x Zr 2 Si x P 3− x O 12 (NZSP) are leading solid electrolyte candidates for sodium‐based energy storage. However, the mechanical properties governing membrane reliability, namely elastic modulus, hardness, fracture toughness, and flexural strength, have not been systematically characterized across the full composition range, owing to confounding effects from porosity, glassy grain‐boundary phases, and ZrO 2 transformation‐induced and grain‐boundary microcracking in conventionally sintered materials. Here, we report the first comprehensive mechanical characterization of high‐purity (total secondary‐phase content < 10%), fully dense NZSP across x = 2.0–2.8, prepared by rapid induction hot‐pressing of powders prepared by solution‐assisted solid‐state reaction. Hot‐pressed samples achieve relative densities exceeding 99%, nanosized grains (150–200 nm), nanosized ZrO 2 particles, and glass‐free grain boundaries across most compositions. Elastic modulus increases from 109 GPa ( x = 2.0) to 124 GPa ( x = 2.8), attributed to progressive replacement of compliant phosphate units by stiffer silicate groups and the corresponding increase in the stiffer rhombohedral phase. Hardness follows the same trend, rising from 7.20 to 9.61 GPa. Fracture toughness falls between 1.0 and 1.5 MPa·m 1/2 . Biaxial flexure strength reaches a maximum of 195 MPa at x = 2.4. The critical grain size for thermal expansion anisotropy‐driven cracking falls from 9 µm ( x = 2) to 0.5 µm ( x = 3), for both phases above the hot‐pressed grain size at every composition.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Effect of compaction load on crystalline characteristics and surface morphology of commercial NASICON (Na₃Zr₂Si₂PO₁₂) pelletsJournal of Materials Science: Materials in Engineering · 2026
- Interplay of Composition, Microstructure, and Ionic Conductivity in NaSICON-Type Solid Electrolytes from Scalable Spray-Flame SynthesisACS Applied Energy Materials · 2026
- Microstructural and Interfacial Engineering of NASICON‐Type Na 1 + x Zr 2 Si x P 3 − x O 12 Electrolytes for Solid‐State Sodium Metal Batteries: A ReviewBatteries & Supercaps · 2026
- Na2Ti3O7-Assisted Grain-Boundary Tailoring of NASICON Electrolytes for Room-to-Subzero-Temperature All-Solid-State Sodium Metal Batteries.Angewandte Chemie (International ed. in English) · 2026
- Sulfur-Induced Lattice Disordering in Halide Electrolytes Enables Superionic Sodium-Ion Conduction.ACS nano · 2026
- Prismatic Na-Ion Coordination in the Sulfide-Chloride Solid Electrolyte Enables Fast Na-Ion Transport.Journal of the American Chemical Society · 2026