Evaluation of Marginal Fit and Bacterial Adhesion at the Zirconia Crown–Titanium Base Abutment Interface
Nagat Areid, Pauliina Moilanen, Joao Pitta, Valeria Moisin, Jenni Hjerppe, Irena Sailer, Jasmina Bijelic‐Donova, Timo Närhi
Key points
From the paper's conclusion- Objectives This study aimed to evaluate the marginal fit and bacterial adhesion on the cement margin of screw‐retained implant zirconia crowns cemented on titanium base (Ti‐base) abutments before and after fatigue loading.
Abstract
Objectives This study aimed to evaluate the marginal fit and bacterial adhesion on the cement margin of screw‐retained implant zirconia crowns cemented on titanium base (Ti‐base) abutments before and after fatigue loading. Materials and Methods Anterior monolithic zirconia crowns (IPS e.max ZirCAD Prime, Ivoclar Vivadent) ( n = 20) were cemented with dual‐curing resin composite cement (RelyX Ultimate, Solventum) on Ti‐base abutments (Titanium base CAD/CAM, GH 2.0 mm, AH 4.3 mm, CONELOG, ALTATEC GmbH) and then screw‐retained to corresponding implants (CONELOG PL 4.3). Sterilized specimens ( n = 5/group) were exposed to Streptococcus mutans (NCTC 10449) and Aggregatibacter actinomycetemcomitans (ATCC 29523), in the presence or absence of saliva. Marginal gap and bacterial adhesion were evaluated with scanning electron microscopy (SEM) before and after fatigue loading. Kruskal–Wallis test was used to determine statistical significance between the mean marginal gap values, and the Wilcoxon Mann–Whitney U ‐test for pairwise comparison, with a significance level of p < 0.05. Results The mean gap widths at the abutment–crown interface were 79 ± 61.5 μm prior to loading and 87 ± 56.6 μm following loading. Fatigue loading did not affect the gap size ( p > 0.05); however, the gap size varied between 13 and 240 μm. SEM observation revealed bacterial adhesion on the crown, abutment, and cement margin across all evaluated materials. A. actinomycetemcomitans appeared to show less adhesion and a less extensive distribution than S. mutans . In addition, saliva‐treated specimens appeared to exhibit a less dense distribution of adherent bacteria than untreated specimens. Fatigue loading led to microcrack formation in the cement layer that may have promoted further bacterial growth and aggregation. Conclusions Within the limitations of this study, no statistically significant effect of fatigue loading on marginal gap size was detected. Bacterial adhesion was observed on all surfaces and accumulated at the cement margin, within the critical transmucosal area. Fatigue‐induced microcracks and variations in gap size may have contributed to bacterial retention and accumulation. Further optimization and standardization of cementation procedures may help reduce marginal gap variability.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Clinical Performance and Failure Mechanisms of Zirconia‐Based Toughened Ceramic CrownsInternational Journal of Applied Ceramic Technology · 2026
- Adhesion of Composite Resin to Additively Manufactured Zirconia Using a Self-Adhesive Resin Cement: Evaluation of Micro-Shear Bond Strength.Polymers · 2026
- "Influence of macroretention in polymer-infiltrated ceramic network- and zirconia crowns and different roughness values of titanium bases on adhesive bond strength of hybrid abutment crowns: an in vitro study".BMC oral health · 2026
- 3D-printing for zirconia abutment manufacturing and screw access hole effect: fatigue behavior of milled zirconia simplified restorations.Odontology · 2026
- In vitro evaluation of Streptococcus mutans adhesion on prefabricated primary crowns using colony-forming unit analysis and scanning electron microscopy: a pilot study.BMC research notes · 2026
- Tensile Retention of Lithium Disilicate and Zirconia Crowns Cemented to One-Piece Zirconia Implants: A Pilot In Vitro Study of Cementation Protocol, Resin Cement, and Micro-CT Cement Morphology.Materials (Basel, Switzerland) · 2026