Corrosion and Wear Behaviour of Eggshell-Derived CDHA-GNP Coatings on Ti-6Al-4V and Ti-6Al-7Nb Alloys by Low-Temperature Pack Cementation
Chandra Shekar Beera, Ramanaiah Nallu
Key points
From the paper's conclusion- This study evaluates eggshell-derived calcium-deficient hydroxyapatite (CDHA) and 0.5 wt.% graphene nanoplatelet (GNP)-reinforced CDHA coatings deposited on Ti-6Al-4V and Ti-6Al-7Nb by low-temperature pack cementation at 800 °C for 2 h under argon.
Abstract
Titanium alloys are widely used for orthopaedic and dental implants, yet surface wear and electrochemical degradation remain important performance concerns. This study evaluates eggshell-derived calcium-deficient hydroxyapatite (CDHA) and 0.5 wt.% graphene nanoplatelet (GNP)-reinforced CDHA coatings deposited on Ti-6Al-4V and Ti-6Al-7Nb by low-temperature pack cementation at 800 °C for 2 h under argon. Surface morphology, phase constitution, composition, Raman features, and supporting surface characteristics were examined. Under dry sliding conditions, the CDHA-GNP-coated specimens exhibited lower specific wear rates than the untreated, oxidized, and CDHA-coated specimens for both Ti-6Al-4V and Ti-6Al-7Nb alloys. A further reduction in specific wear rate was observed under saline sliding in 0.9 wt.% NaCl, demonstrating the favourable wear response of the GNP-containing coatings under both sliding environments. SEM examination of the worn surfaces showed comparatively reduced surface damage and more compacted wear regions for the CDHA-GNP coatings. These observations are consistent with the lower material removal observed for the GNP-containing coatings and indicate their improved resistance to sliding wear under both dry and saline conditions. While the potentiodynamic polarization in 3.5 wt.% NaCl. For the CDHA-GNP condition, I_corr decreased from 8.822 to 5.275 µA cm⁻² for Ti-6Al-4V and from 7.974 to 4.489 µA cm⁻² for Ti-6Al-7Nb, corresponding to reductions of 40.2% and 43.7%, respectively. The corresponding corrosion rates decreased from 0.0782 to 0.0467 mm y⁻¹ and from 0.0692 to 0.0390 mm y⁻¹, representing reductions of 40.3% and 43.6%. The results demonstrate the measured wear and electrochemical responses under the investigated laboratory conditions, while adhesion, fatigue, long-term stability, and biological performance require further validation.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Influence of Graphene Oxide and Palladium Incorporation on Hydrothermally Grown Hydroxyapatite Coatings on β-Ti30Zr5Mo Alloy: Surface Chemistry, Corrosion and Biological Performance.Materials (Basel, Switzerland) · 2026
- Tailoring the Surface Performance of Near-β Ti-13Nb-13Zr Alloy Through TaN/Au Bilayer Coatings: Electrochemical Stability, Tribocorrosion Mechanisms and BiocompatibilitySolids · 2026
- Investigation of the Corrosion and Wear Behavior of Electrochemically Deposited Zn-Co-Graphene-TiO2 Nanocomposite Coatings on Ti6Al4V Substrates Fabricated by Selective Laser Melting (SLM).Materials (Basel, Switzerland) · 2026
- Interface‐Engineered Graphene‐Coated Titanium Dioxide Nanoparticles for High‐Performance Grease LubricationAdvanced Materials Interfaces · 2026
- Development of sol-gel derived fluoridated hydroxyapatite/CaTiO3 composite coating on titanium implant.Journal of materials science. Materials in medicine · 2026
- Improvement of Electrochemical Behavior of Nitinol by Hydroxyapatite–Tantalum Oxide Coating Fabricated via Electrophoretic Deposition for Biomedical Applicationsنشریه علمی پژوهشی مواد پیشرفته در مهندسی · 2026