Engineering Research Express

Life Cycle Assessment of Reinforced Concrete Structures using Pozzolanic Materials

Ali Danandeh Mehr, Emirhan Yener, Kaan Beyazkılıç

Key points

From the paper's conclusion
  • The results, quantified through service life level indicators, indicated that at 50 mm cover, replacing 40% of cement with a pozzolan mix containing 10% silica fume, 15% slag, and 15% fly ash offers the greatest carbon reduction, although multi-category results reveal significant environmental trade-offs regarding toxicity.

Abstract

Sustainability goals and stricter environmental protection requirements now guide a wide range of experts, from material scientists to architects, to find practical ways to incorporate byproducts and waste materials into concrete construction. The urgent focus on climate change has led researchers to investigate materials, such as polymers and pozzolans, as additives, offering ecological solutions to reduce heavy cement use and lower carbon emissions from concrete structures. This study explores the effects of supplementary cementitious materials, specifically fly ash, ground granulated blast-furnace slag, and silica fume, on delaying chlorideinduced corrosion initiation and influencing service-life outcomes under Mediterranean marine chloride conditions. Life-365 is employed to conduct a comparative service-life assessment using a realistic dynamic diffusion approach, combined with a multi-category life cycle assessment framework to facilitate interpretation beyond a single climate indicator. The analysis has been adapted to the conditions of the Antalya coastal region, considering seasonal temperature fluctuations to reflect sensitivity to chloride flow. The results, quantified through service life level indicators, indicated that at 50 mm cover, replacing 40% of cement with a pozzolan mix containing 10% silica fume, 15% slag, and 15% fly ash offers the greatest carbon reduction, although multi-category results reveal significant environmental trade-offs regarding toxicity. Additionally, increasing concrete cover from 30 mm to 50 mm consistently prolongs 2 the predicted time to corrosion initiation and extends overall service life across all mixtures, with the degree of improvement heavily depending on binder composition.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers

Life Cycle Assessment of Reinforced Concrete Structures using Pozzolanic Materials — Science Skim