Characterization of L-PBF Printed AISI 316L Parts: Dimensional accuracy, surface quality, microstructural and mechanical behaviors
Aysu Hande Yucel, Ali Taner Kuzu, Rasid Ahmed Yildiz, Mohammad Malekan, Mustafa Bakkal
Key points
From the paper's conclusion- Therefore, the suitability of this condition for preliminary prototyping should be assessed against the dimensional tolerances and functional requirements of the intended application rather than assumed to be universally acceptable.
Keywords: Laser powder bed fusion, Surface roughness, Computed tomography, Mechanical properties, dimensional accuracy.
Abstract
This study investigates components manufactured using low volumetric energy density (VED) in laser powder bed fusion (L-PBF) additive manufacturing, specifically for preliminary prototyping. In industrial contexts, tangible prototypes play a vital role in identifying potential design flaws before assembly and production. To evaluate the influence of low and high VEDs, AISI 316L stainless steel specimens were produced at two speeds while maintaining constant laser power: 300 mm/s and 1500 mm/s, corresponding to VEDs of 80 J/mm³ (high-VED) and 16 J/mm³ (low-VED), respectively. Only the scanning speed was varied, while the laser power (90 W), hatch distance (150 µm), and layer thickness (25 µm) were kept constant. The effect of scanning speed, expressed through VED, was evaluated on four responses: geometric accuracy, surface roughness, porosity, and mechanical properties. Increasing VED from 16 to 80 J/mm³ increased the flatness deviation of all matchbox specimens, mostly for the 2.3 mm-thick specimen (from approximately 1.71% to 6.96%), and increased the angular deviation of the triangular prisms by approximately 1.18–6.88 pp, depending on the angle. In contrast, circularity deviations decreased slightly for all cylindrical features, with the largest decrease observed on the outer surface of the smaller hollow tube (with an inner radius of 1.4 mm and an outer radius of 2.3 mm) from 5.05% to 4.07%, while cylindricity exhibited a more geometry-dependent response for the same tube, decreasing from 30.45% to 28.81%. Surface roughness decreased by approximately 40% at higher VED, with Ra decreasing from 13.41 to 8.03 µm for the dogbone specimens and from 17.05 to 9.98 µm for the hemisphere specimens. Micro-computed tomography revealed substantially higher XCT-resolved porosity in the low-VED specimen (~1.49%) compared with the high-VED specimen (0.17%). Tensile testing showed that the specimen produced at 80 J/mm³ achieved an ultimate tensile strength of 684.0 ± 7.2 MPa, compared with 120.5 ± 16.2 MPa for the specimen produced at 16 J/mm³, corresponding to an approximately 5.7-fold increase. Under the low-VED condition, flatness deviations ranged from approximately 1.71% to 6.11% and angular deviations from 4.68% to 15.16%. The fivefold increase in scanning speed reduces scanning time but compromises density, surface quality, and strength. Therefore, the suitability of this condition for preliminary prototyping should be assessed against the dimensional tolerances and functional requirements of the intended application rather than assumed to be universally acceptable. Keywords: Laser powder bed fusion, Surface roughness, Computed tomography, Mechanical properties, dimensional accuracy.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Correlations in LPBF-fabricated Ti6Al4V: Influence of laser power and scanning speed on microstructure and mechanical performanceResults in Engineering · 2026
- Beyond Volumetric Energy Density: Process-Window Mapping and Density Metrology for Laser Powder Bed Fusion of High-Strength A20X Aluminium and 304L Stainless SteelJournal of Manufacturing and Materials Processing · 2026
- Role of laser beam shape and energy density in modulating surface quality, porosity, microstructure, and mechanical properties of PBF-LB/M Ti-6Al-4VJournal of Materials Processing Technology · 2026
- Optimization of laser powder bed fusion process to enhance mechanical properties of as-built Ti–6Al–4V samplesJournal of Materials Research and Technology · 2025
- Investigating microstructural and mechanical property uniformity in 316L stainless steel alloys processed via laser powder bed fusion processMaterials Science and Engineering A · 2026
- Experimental and Simulation-Based Assessment of Dimensional Accuracy and Thermomechanical Properties of AlSi10Mg Cubes Produced by LPBFMaterials & Design · 2025