AZO emerges as a viable challenger to ITO under identical RF sputtering conditions assessed through the Haacke high-resolution figure of merit and Zanatta disorder analysis
Diana Pineda-Vázquez, Alejandro Reyes-Coronado, Arturo Rodríguez-Gómez
Key points
From the paper's conclusion- We examined how RF power (50 and 150 W) and substrate temperature (room temperature and 300 ∘ C) shape the structural, optical, and electronic-transport properties of the three oxides.
Abstract
Transparent conducting oxides (TCOs) reconcile efficient electrical conduction with high visible transparency. Yet comparisons between competing TCOs remain confounded, since each oxide is optimized in its own processing window, so its performance reflects the fabrication route rather than the intrinsic merit of the material. Here we propose that this ambiguity could be resolved by depositing indium tin oxide (ITO), aluminium-doped zinc oxide (AZO), and undoped zinc oxide (ZnO) within a single shared window of non-reactive radio-frequency (RF) magnetron sputtering on fused silica and soda-lime glass substrates. The common processing window provides a controlled comparison of the three oxides, with undoped ZnO as the reference for AZO; it does not imply that each material is individually optimized. We examined how RF power (50 and 150 W) and substrate temperature (room temperature and 300 ∘ C) shape the structural, optical, and electronic-transport properties of the three oxides. X-ray diffraction and field-emission scanning electron microscopy revealed material-dependent structural and morphological responses, including a bimodal grain-size distribution in AZO deposited at 150 W and 300 ∘ C. Comparative Tauc and Zanatta analyses revealed method-dependent optical gaps, while the fitted broadening parameter δ E provided a complementary descriptor of the absorption-edge width. Van der Pauw Hall measurements showed that ITO at 150 W and 300 ∘ C reached the highest optoelectronic quality, with a Haacke high-resolution figure of merit Φ H − HR = 0.720, a sheet resistance of 7.84 Ω / ◻ , and an average visible transmittance T avg 88.51%, while AZO at the same conditions reached Φ H-HR = 0.560, a sheet resistance of 63.1 Ω / ◻ , and T avg = 85.04%. Crucially, under identical deposition conditions, AZO emerged as a competitive, indium-free challenger ( Φ H − HR = 0.562; R s = 63.1 Ω / ◻ ), a viable alternative to ITO when materials are judged on a truly equal footing.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Effect of Thin Film Deposition Method on Growth, Structural, and Optical Properties of ZnO:Al FilmsChemistrySelect · 2026
- Optimization of RF Sputtering Power for High-Performance ITZO Thin-Film Transistors: Correlation Between Film Properties, Oxygen Defects and Electrical PerformanceInorganics · 2026
- Systematic Optimization of Sputtered AZO Thin Films and Their Integration as Alternative Transparent Electrodes for Perovskite Solar Cells.ACS omega · 2026
- From Transparency to Transport: Optoelectronic and Interfacial Signatures of n-Type ITO, FTO, ZnO and TiO2 Semiconductors.Molecules (Basel, Switzerland) · 2026
- Effects of Al contents on the electrical performance and low-frequency noise properties of InAlZnO thin-film transistorsApplied Physics Letters · 2025
- Annealing-Temperature-Dependent Electrical and Optical Performance of Solution-Processed Amorphous IGZO TFTsTechnologies · 2026